3-D Simulation of AC Loss in a 114-Filament MgB <sub>2</sub> Wire at 20 K
In future electric aircraft applications employing all-superconducting rotating machines, round multifilamentary magnesium diboride (MgB<sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub>) wires are a preferrable material for lowering AC loss, due to their small filaments at the macron level and tight twist pitch. Our previous work has investigated AC loss behaviour in a 54-filament MgB<sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> wire with a filament radius of 12.5 μm, where the filament size was found not ideal for loss reduction. In this work, 3D AC loss simulations of a twisted, non-magnetic 114-filament MgB<sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</sub> wire with a 5 μm filament radius at 20 K are performed using <italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">H</i>-formulation. Three types of AC losses are studied: (1) transport loss only (<italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Q</i><sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">t0</sub>, with current levels up to 90% of its self-field critical current <italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">I</i><sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">c0</sub>), (2) magnetization loss only (<italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Q</i><sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">m0</sub>, with AC field amplitudes and frequencies up to 2 T and 200 Hz, respectively), (3) total AC loss carrying AC current exposed to AC field (<italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Q</i><sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">total</sub>, with AC field also up to 2 T and current levels up to 40% of <italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">I</i><sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">c0</sub>). Simulation results show that, for the <italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Q</i><sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">m0</sub>, the simulated hysteresis loss <italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Q</i><sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">h</sub> of a 5-mm twist pitch, 114-filament wire at 50 Hz and 200 Hz matches the analytical hysteresis loss equation for a cylindrical superconductor, scaled by 114 (the number of filaments), when <italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">B</i><sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">m</sub> ≤ 0.5 T. Increasing the twist pitch (5 mm Vs 10 mm) and filament size (5 μm in the 114-filament wire Vs 12.5 μm in the 54-filament wire) leads to a higher <italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Q</i><sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">m0</sub> due to the coupling effect. Moreover, the simulated <italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Q</i><sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">total</sub> of the 114-filament wire range from 0.22 to 7.48 W/cm3 for <italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">i</i> ≤ 0.4 and <italic xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">B</i><sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">m</sub> ≤ 0.5 T operated at 200 Hz.
Authors
- Zhenan Jiang (ORCID: https://orcid.org/0000-0002-3482-3510)
- Strickland Nick
- Yukai Qiao (ORCID: https://orcid.org/0000-0003-1711-9860)
- Rodney A. Badcock
- Matt Rindfleisch
- Mark Ainslie
- Yueming Sun
Institutions
- Victoria University of Wellington (NZ)
- King's College School (GB)
- Hyper Tech Research (United States) (US)
Publication Details
- Journal
- IEEE Transactions on Applied Superconductivity
- Published
- 2026-01-30
- DOI
- https://doi.org/10.1109/tasc.2026.3659823
- Primary Topic
- Superconductivity in MgB2 and Alloys
- Type
- article
- Field-Weighted Citation Impact
- 0.00