Room-Temperature Gas Adsorption on Standing and Zigzag ZnO Nanowires: A ReaxFF-MD Study

Gas adsorption is intrinsically governed by the surface structure of sensing materials, where a large surface area and a high reactivity are critical for optimal performance. Nanostructured materials, with their exceptional surface-to-volume ratios, offer enhanced sensing capabilities. In this study, we designed two distinct ZnO nanowire morphologies (standing and zigzag) and used reactive force field molecular dynamics (ReaxFF-MD) simulations to evaluate their adsorption performance for O<sub>2</sub>, H<sub>2</sub>, Cl<sub>2</sub>, CH<sub>2</sub>O, C<sub>2</sub>H<sub>6</sub>O, and C<sub>3</sub>H<sub>6</sub>O at 300 K with an initial gas level of 200 molecules per system. The results show that all molecules fully adsorb on the ZnO nanowire surfaces, O<sub>2</sub> dissociates into O atoms, and C<sub>2</sub>H<sub>6</sub>O dissociates into C<sub>2</sub>H<sub>5</sub>O and H atoms, both attached to the surface. Energy analysis shows that standing nanowires exhibit more negative adsorption energies for nonpolar gases (O<sub>2</sub>, -10317.26 kcal/mol; H<sub>2</sub>, -385.67 kcal/mol; Cl<sub>2</sub>, -19000 kcal/mol), whereas zigzag nanowires favor polar molecules (CH<sub>2</sub>O, -9380 kcal/mol; C<sub>2</sub>H<sub>6</sub>O, -8568.58 kcal/mol; C<sub>3</sub>H<sub>6</sub>O, -6897.73 kcal/mol). Both morphologies display a two-stage adsorption process, with adsorption numbers in the second stage decreasing in the following order: O<sub>2</sub> > C<sub>2</sub>H<sub>6</sub>O > CH<sub>2</sub>O > C<sub>3</sub>H<sub>6</sub>O > Cl<sub>2</sub> > H<sub>2</sub>. Compared to zigzag nanowires, standing nanowires adsorb 136 O<sub>2</sub>, 9 H<sub>2</sub>, 15 Cl<sub>2</sub>, 38 CH<sub>2</sub>O, 53 C<sub>2</sub>H<sub>6</sub>O, and 29 C<sub>3</sub>H<sub>6</sub>O molecules, whereas zigzag nanowires adsorb 129 O<sub>2</sub>, 10 H<sub>2</sub>, 18 Cl<sub>2</sub>, 37 CH<sub>2</sub>O, 44 C<sub>2</sub>H<sub>6</sub>O, and 27 C<sub>3</sub>H<sub>6</sub>O molecules. In both morphologies, O<sub>2</sub> adsorption leads to a strong improvement in sensitivity. These results pave the way for smarter nanoscale designs in next-generation gas sensors.

Authors

Institutions

Publication Details

Journal
Langmuir
Published
2026-01-21
DOI
https://doi.org/10.1021/acs.langmuir.5c04851
Primary Topic
ZnO doping and properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Room-Temperature Gas Adsorption on Standing and Zigzag ZnO Nanowires: A ReaxFF-MD Study

QingXiang Liu, Yang Yu, Waleed Ftahi, Yuxiang Ni et al.
Langmuir
ZnO doping and properties
article

Room-Temperature Gas Adsorption on Standing and Zigzag ZnO Nanowires: A ReaxFF-MD Study

QingXiang Liu, Yang Yu, Waleed Ftahi, Yuxiang Ni, Nusaibah AL-Shaeri, Yongliang Tang
article en

Abstract

Gas adsorption is intrinsically governed by the surface structure of sensing materials, where a large surface area and a high reactivity are critical for optimal performance. Nanostructured materials, with their exceptional surface-to-volume ratios, offer enhanced sensing capabilities. In this study, we designed two distinct ZnO nanowire morphologies (standing and zigzag) and used reactive force field molecular dynamics (ReaxFF-MD) simulations to evaluate their adsorption performance for O<sub>2</sub>, H<sub>2</sub>, Cl<sub>2</sub>, CH<sub>2</sub>O, C<sub>2</sub>H<sub>6</sub>O, and C<sub>3</sub>H<sub>6</sub>O at 300 K with an initial gas level of 200 molecules per system. The results show that all molecules fully adsorb on the ZnO nanowire surfaces, O<sub>2</sub> dissociates into O atoms, and C<sub>2</sub>H<sub>6</sub>O dissociates into C<sub>2</sub>H<sub>5</sub>O and H atoms, both attached to the surface. Energy analysis shows that standing nanowires exhibit more negative adsorption energies for nonpolar gases (O<sub>2</sub>, -10317.26 kcal/mol; H<sub>2</sub>, -385.67 kcal/mol; Cl<sub>2</sub>, -19000 kcal/mol), whereas zigzag nanowires favor polar molecules (CH<sub>2</sub>O, -9380 kcal/mol; C<sub>2</sub>H<sub>6</sub>O, -8568.58 kcal/mol; C<sub>3</sub>H<sub>6</sub>O, -6897.73 kcal/mol). Both morphologies display a two-stage adsorption process, with adsorption numbers in the second stage decreasing in the following order: O<sub>2</sub> > C<sub>2</sub>H<sub>6</sub>O > CH<sub>2</sub>O > C<sub>3</sub>H<sub>6</sub>O > Cl<sub>2</sub> > H<sub>2</sub>. Compared to zigzag nanowires, standing nanowires adsorb 136 O<sub>2</sub>, 9 H<sub>2</sub>, 15 Cl<sub>2</sub>, 38 CH<sub>2</sub>O, 53 C<sub>2</sub>H<sub>6</sub>O, and 29 C<sub>3</sub>H<sub>6</sub>O molecules, whereas zigzag nanowires adsorb 129 O<sub>2</sub>, 10 H<sub>2</sub>, 18 Cl<sub>2</sub>, 37 CH<sub>2</sub>O, 44 C<sub>2</sub>H<sub>6</sub>O, and 27 C<sub>3</sub>H<sub>6</sub>O molecules. In both morphologies, O<sub>2</sub> adsorption leads to a strong improvement in sensitivity. These results pave the way for smarter nanoscale designs in next-generation gas sensors.

LangmuirVol. 42(4)
Sichuan University (CN), Southwest Jiaotong University (CN)
Affordable and clean energy
Openalex Percentile: Top 81%
ZnO doping and properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.