Unveiling the Formation of Inclusions and Their Impact on Scintillation Performance in Sr Codoped LaBr <sub>3</sub> :5%Ce Crystals

Sr2+ codoped LaBr3:Ce3+ scintillation crystals exhibit exceptional performance in various radiation detection applications, achieving near-theoretical energy resolution (2%) through optimized codoping strategies. However, the substantial doping concentrations required (0.35–0.7 mol %) introduce significant challenges in crystal growth, particularly defect formation, which limits large-scale production and practical application. Herein, this study investigates SrBr2-induced defect dynamics during crystal growth with a focus on the role of inclusion defects in degrading scintillation performance. The inclusion density increases along the crystal growth direction and follows the matrix-controlled morphological evolution, eventually forming well-defined polyhedral morphologies with equilibrium hexagonal prism bounded by {1000} and {1010} facets. Constitutional supercooling-induced interface instabilities emerge as the primary mechanism driving inclusion formation. Crucially, increasing inclusion density along the growth direction leads to enhanced photon scattering, significantly reducing transmittance, light output, and energy resolution─from 2.69 to 5.9%. In addition, the scattering of scintillation photons by inclusion introduced an additional slow decay component in the scintillation time profile. By leveraging these insights, we optimized growth parameters to suppress this instability, achieving improved crystal quality with an energy resolution of 2.44%@662 keV─a significant improvement compared to conventional methods. These observations quantitatively reveal the influence of macroscopic inclusions, establish a comprehensive framework for macroscopic defect engineering in LaBr3-based scintillators, and further provide effective strategies for control and optimization of metal halide scintillators.

Authors

Institutions

Publication Details

Journal
Crystal Growth & Design
Published
2026-01-22
DOI
https://doi.org/10.1021/acs.cgd.5c00968
Primary Topic
Radiation Detection and Scintillator Technologies
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Unveiling the Formation of Inclusions and Their Impact on Scintillation Performance in Sr Codoped LaBr 3 :5%Ce Crystals

W JIE, Xianggang Zhang, Dan Zheng, Baoqiang Zhang et al.
Crystal Growth & Design
Radiation Detection and Scintillator Technologies
article

Unveiling the Formation of Inclusions and Their Impact on Scintillation Performance in Sr Codoped LaBr 3 :5%Ce Crystals

W JIE, Xianggang Zhang, Dan Zheng, Baoqiang Zhang, Ning Han, Qinghua Zhao, Ziang Yin, Kejing Liu, Suyu Chen, Zhe Kang, Jian Li, Tao Wang, Jinbo Liu
article en

Abstract

Sr2+ codoped LaBr3:Ce3+ scintillation crystals exhibit exceptional performance in various radiation detection applications, achieving near-theoretical energy resolution (2%) through optimized codoping strategies. However, the substantial doping concentrations required (0.35–0.7 mol %) introduce significant challenges in crystal growth, particularly defect formation, which limits large-scale production and practical application. Herein, this study investigates SrBr2-induced defect dynamics during crystal growth with a focus on the role of inclusion defects in degrading scintillation performance. The inclusion density increases along the crystal growth direction and follows the matrix-controlled morphological evolution, eventually forming well-defined polyhedral morphologies with equilibrium hexagonal prism bounded by {1000} and {1010} facets. Constitutional supercooling-induced interface instabilities emerge as the primary mechanism driving inclusion formation. Crucially, increasing inclusion density along the growth direction leads to enhanced photon scattering, significantly reducing transmittance, light output, and energy resolution─from 2.69 to 5.9%. In addition, the scattering of scintillation photons by inclusion introduced an additional slow decay component in the scintillation time profile. By leveraging these insights, we optimized growth parameters to suppress this instability, achieving improved crystal quality with an energy resolution of 2.44%@662 keV─a significant improvement compared to conventional methods. These observations quantitatively reveal the influence of macroscopic inclusions, establish a comprehensive framework for macroscopic defect engineering in LaBr3-based scintillators, and further provide effective strategies for control and optimization of metal halide scintillators.

Crystal Growth & DesignVol. 26(3)
Northwestern Polytechnical University (CN), Crystal Research (United States) (US), Research & Development Institute (US), IS Instruments (United Kingdom) (GB), State Key Laboratory of Solidification Processing, Ministry of Industry and Information Technology (CN)
Affordable and clean energy
Openalex Percentile: Top 80%
Radiation Detection and Scintillator Technologies
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.