Renewable bis-benzoxazine from symmetrical vanillin-based dimer

A novel renewable bis-benzoxazine has been created using a Vanillin-based dimer, furfurylamine and paraformaldehyde through a Mannich reaction. The Molecular structure of the synthesized bis-benzoxazine monomer was analyzed using Nuclear Magnetic Resonance spectroscopy and Fourier Transform infrared spectroscopy. The curing behavior of the bis-benzoxazine was evaluated by Differential Scanning Calorimetry and in situ FT-IR. The curing reaction exhibited a peak temperature of 228°C and a relatively low heat of reaction at 85 J/g. The thermal stability of the resulting polybenzoxazine was examined using thermogravimetric Analysis (TGA), which indicated a low degradation rate between 300°C and 800°C, along with a high char yield at 800°C. Pyrolysis-Gas Chromatography/Mass Spectrometry (Py-GC/MS) analysis revealed that the primary pyrolysis products of polybenzoxazine were phenol and furan derivatives.

Authors

Institutions

Publication Details

Journal
High Performance Polymers
Published
2026-01-12
DOI
https://doi.org/10.1177/09540083251358883
Primary Topic
Epoxy Resin Curing Processes
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Renewable bis-benzoxazine from symmetrical vanillin-based dimer

Jilei Xu, Youxun Dai, Chunxia Zhao, Hui Li
High Performance Polymers
Epoxy Resin Curing Processes
article

Renewable bis-benzoxazine from symmetrical vanillin-based dimer

Jilei Xu, Youxun Dai, Chunxia Zhao, Hui Li
article en

Abstract

A novel renewable bis-benzoxazine has been created using a Vanillin-based dimer, furfurylamine and paraformaldehyde through a Mannich reaction. The Molecular structure of the synthesized bis-benzoxazine monomer was analyzed using Nuclear Magnetic Resonance spectroscopy and Fourier Transform infrared spectroscopy. The curing behavior of the bis-benzoxazine was evaluated by Differential Scanning Calorimetry and in situ FT-IR. The curing reaction exhibited a peak temperature of 228°C and a relatively low heat of reaction at 85 J/g. The thermal stability of the resulting polybenzoxazine was examined using thermogravimetric Analysis (TGA), which indicated a low degradation rate between 300°C and 800°C, along with a high char yield at 800°C. Pyrolysis-Gas Chromatography/Mass Spectrometry (Py-GC/MS) analysis revealed that the primary pyrolysis products of polybenzoxazine were phenol and furan derivatives.

High Performance Polymers
Southwest Petroleum University (CN)
Affordable and clean energy
Openalex Percentile: Top 89%
Epoxy Resin Curing Processes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.