Controlling Jahn–Teller Distortion through Mn Slab Localization for Stable High-Voltage Sodium-Ion Batteries
Mn-rich layered oxides are among the most promising cathode materials for large-scale sodium-ion batteries due to their high capacity, elemental abundance, and low cost. Nevertheless, the practical application of these materials is impeded by the pronounced and intractable Jahn-Teller effect associated with Mn<sup>3+</sup> ions. This effect triggers cooperative lattice distortion, resulting in structural degradation and compromised cycling stability. In this work, we demonstrate that spatially localizing Jahn-Teller active Mn<sup>3+</sup> ions within confined Mn-rich slabs effectively suppresses long-range distortion and stabilizes the layered framework. The engineered Mn-rich oxide, NaNi<sub>0.3</sub>Cu<sub>0.1</sub>Mn<sub>0.6</sub>O<sub>2</sub> (NCM316), exhibits exceptional electrochemical performance, achieving 89.5% voltage retention after 200 cycles. In full-cell configurations, NCM316 delivers a high discharge voltage of 3.36 V, the highest reported for Mn-based layered cathodes, while maintaining 84% capacity retention after 500 cycles and reaching an energy density of 337 Wh kg<sup>-1</sup>, outperforming all other Mn-based layered cathodes under a high cutoff voltage of 4.4 V. Comprehensive characterization using synchrotron X-ray and neutron scattering techniques, supported by theoretical simulations, confirm the localized presence of Mn<sup>3+</sup> and elucidate its role in maintaining structural integrity and mitigating adverse interactions with neighboring transition metals. This work offers insight into the mechanism of Jahn-Teller distortion in Mn-rich layered oxides and proposes a broadly applicable design principle for stabilizing other Jahn-Teller active systems, such as layered lithium-rich cathodes, spinel-type oxides, and manganese-based materials for aqueous batteries.
Authors
- H. Can Chen
- J. B. Kim
- Bernt Johannessen (ORCID: https://orcid.org/0000-0002-3027-0816)
- Peng Li (ORCID: https://orcid.org/0000-0003-3497-1887)
- Wen Hui Yin (ORCID: https://orcid.org/0000-0002-7110-9471)
- Yameng Fan
- Wei Kong Pang
- Wang Hay Kan
- Tianyi Ma
- Xinghan Li
- Baohua Jia
- Mingyue Wang
- Haobo Li
- Xiaobo Zheng
- Xiaoning Li
- Lingfei Zhao
Institutions
- University of Technology Sydney (AU)
- Australian Nuclear Science and Technology Organisation (AU)
- Nanyang Technological University (SG)
- Chinese Academy of Sciences (CN)
- University of Wollongong (AU)
- Australian Synchrotron (AU)
- MIT University (MK)
- China Spallation Neutron Source (CN)
- Physical Sciences (United States) (US)
- Intelligent Energy (United Kingdom) (GB)
- Mayaterials (United States) (US)
- Clean Energy (United States) (US)
- Superconducting Systems (United States) (US)
- Spallation Neutron Source
- RMIT University (AU)
Publication Details
- Journal
- ACS Nano
- Published
- 2025-12-31
- DOI
- https://doi.org/10.1021/acsnano.5c17738
- Primary Topic
- Advancements in Battery Materials
- Type
- article
- Field-Weighted Citation Impact
- 0.00