The effect of carbonate energizer on pack carburizing ASTM A36 steel

Pack carburizing process of carbon steel, energizer plays an important role in the changes in surface hardness, carburized layer and microstructure of carbon steel. A study has been conducted on changes in surface hardness and microstructure of ASTM A36 low carbon steel due to the pack carburizing process with variations of energizer. The pack carburizing treatment process was carried out at a temperature of 900 ℃ and soaking time of 2 hours. The carburizing media was a mixture of charcoal powder and energizer with a ratio of 70: 30 weight percentage, with heating carried out in an electric furnace. The energizer used was carbonate energizer in the form of CaCO3, BaCO3, and Na2CO3. The results of the study surface hardness, microstructure and thickness of carburized layer of ASTM A36 steel specimen after pack carburizing treatment are influenced by energizer. The use of CaCO3 energizer has the greatest impact on increasing surface hardness, microstructure and thickness of carburized layer of ASTM A36 steel specimen, which was pack carburized.

Institutions

Publication Details

Journal
Zenodo (CERN European Organization for Nuclear Research)
Published
2025-05-31
DOI
https://doi.org/10.5281/zenodo.17748453
Primary Topic
Microstructure and Mechanical Properties of Steels
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

The effect of carbonate energizer on pack carburizing ASTM A36 steel

Zenodo (CERN European Organization for Nuclear Research)
Microstructure and Mechanical Properties of Steels
article

The effect of carbonate energizer on pack carburizing ASTM A36 steel

article en

Abstract

Pack carburizing process of carbon steel, energizer plays an important role in the changes in surface hardness, carburized layer and microstructure of carbon steel. A study has been conducted on changes in surface hardness and microstructure of ASTM A36 low carbon steel due to the pack carburizing process with variations of energizer. The pack carburizing treatment process was carried out at a temperature of 900 ℃ and soaking time of 2 hours. The carburizing media was a mixture of charcoal powder and energizer with a ratio of 70: 30 weight percentage, with heating carried out in an electric furnace. The energizer used was carbonate energizer in the form of CaCO3, BaCO3, and Na2CO3. The results of the study surface hardness, microstructure and thickness of carburized layer of ASTM A36 steel specimen after pack carburizing treatment are influenced by energizer. The use of CaCO3 energizer has the greatest impact on increasing surface hardness, microstructure and thickness of carburized layer of ASTM A36 steel specimen, which was pack carburized.

Zenodo (CERN European Organization for Nuclear Research)
University of Mataram (ID)
Openalex Percentile: Top 49%
Microstructure and Mechanical Properties of Steels
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.