Formation Mechanism and Kinetics of NO<sub>x</sub> in Sintering Process

Iron ore powder is the main source of NOx in the sintering process. The existing end treatment technology is difficult to cure environmental hazards due to high cost and secondary pollution. Therefore, in this study, through the NOx generation experiments and mechanism analysis of five kinds of iron ore powder, the low emission characteristic ore powder was selected for actual production. The results show that the NOx emission concentration of different iron ore powders varies with temperature. As the temperature increases, the peak concentration of NOx becomes larger, the peak time becomes shorter, and the harm becomes greater. Among them, the process concentration and peak concentration of Sijiaying powder are relatively low in the sintering process. The pre-exponential coefficient and activation energy of the apparent rate of NO formation interface reaction, the pre-exponential coefficient of the effective diffusion coefficient of gas diffusion in the product layer, and the activation energy of atomic movement are the lowest.

Institutions

Publication Details

Journal
ISIJ International
Published
2025-11-04
DOI
https://doi.org/10.2355/isijinternational.isijint-2025-258
Primary Topic
Iron and Steelmaking Processes
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Formation Mechanism and Kinetics of NOx in Sintering Process

ISIJ International
Iron and Steelmaking Processes
article

Formation Mechanism and Kinetics of NOx in Sintering Process

article en

Abstract

Iron ore powder is the main source of NOx in the sintering process. The existing end treatment technology is difficult to cure environmental hazards due to high cost and secondary pollution. Therefore, in this study, through the NOx generation experiments and mechanism analysis of five kinds of iron ore powder, the low emission characteristic ore powder was selected for actual production. The results show that the NOx emission concentration of different iron ore powders varies with temperature. As the temperature increases, the peak concentration of NOx becomes larger, the peak time becomes shorter, and the harm becomes greater. Among them, the process concentration and peak concentration of Sijiaying powder are relatively low in the sintering process. The pre-exponential coefficient and activation energy of the apparent rate of NO formation interface reaction, the pre-exponential coefficient of the effective diffusion coefficient of gas diffusion in the product layer, and the activation energy of atomic movement are the lowest.

ISIJ InternationalVol. 65(13)
North China University of Science and Technology (CN)
Openalex Percentile: Top 51%
Iron and Steelmaking Processes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics