HEAT TREATMENT OPTIMIZATION ON THE WEAR BEHAVIOR OF A LOW STEEL NI-B-CNT ELECTROLESS COATING ALLOY

ABSTRACT: This work aimed to conduct a statistical analysis of the influence of heating treatment. Using the response surface methodology (RSM) technique, which is based on a core composite design, factors such as temp, deposition duration, and amount of CNTs on the wear behavior of electroless coatings (Ni-B-CNT and Ni-B) on low-alloy steels were investigated. The impacts of the heating treatment temp and deposition duration on the wear rate were evaluated for specimens heated to various CNT amounts (0, 35, and 0.7%). Specimen wear is accelerated by increasing the temperature and deposition duration between 350 and 400 degrees Celsius and then increasing the deposition temperature between 400 and 450 degrees Celsius. The wear rate of materials depends on several material and feature properties, including the topography, hardness, and frictional coefficient, in addition to the wear test conditions.

Publication Details

Journal
Zenodo (CERN European Organization for Nuclear Research)
Published
2025-09-28
DOI
https://doi.org/10.5281/zenodo.17218204
Primary Topic
Mycotoxins in Agriculture and Food
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

HEAT TREATMENT OPTIMIZATION ON THE WEAR BEHAVIOR OF A LOW STEEL NI-B-CNT ELECTROLESS COATING ALLOY

Zenodo (CERN European Organization for Nuclear Research)
Mycotoxins in Agriculture and Food
article

HEAT TREATMENT OPTIMIZATION ON THE WEAR BEHAVIOR OF A LOW STEEL NI-B-CNT ELECTROLESS COATING ALLOY

article en

Abstract

ABSTRACT: This work aimed to conduct a statistical analysis of the influence of heating treatment. Using the response surface methodology (RSM) technique, which is based on a core composite design, factors such as temp, deposition duration, and amount of CNTs on the wear behavior of electroless coatings (Ni-B-CNT and Ni-B) on low-alloy steels were investigated. The impacts of the heating treatment temp and deposition duration on the wear rate were evaluated for specimens heated to various CNT amounts (0, 35, and 0.7%). Specimen wear is accelerated by increasing the temperature and deposition duration between 350 and 400 degrees Celsius and then increasing the deposition temperature between 400 and 450 degrees Celsius. The wear rate of materials depends on several material and feature properties, including the topography, hardness, and frictional coefficient, in addition to the wear test conditions.

Zenodo (CERN European Organization for Nuclear Research)
Openalex Percentile: Top 34%
Mycotoxins in Agriculture and Food
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.