The fast volumetric deposition of multi-MeV high current runaway electron (RE) beams constitutes the most critical issue for the ITER tungsten (W) first wall (FW) longevity. Such relativistic electron beams could generate extreme volumetric power densities inside the FW armour which lead to significant vaporization, deep melting and even material explosions, as well as to elevated temperatures at the bond interface with the cooling substrate that could cause rupture and water leaks. Here the thermal response of the ITER FW is modeled with a three-stage, one-way coupled workflow focusing on assessments of the extent of the wall damage and the increase of the bond interface temperature for varying W thickness. Increased W thickness is found to be essential for wall protection against intense RE dissipation events in terms of both W tile damage and cooling system integrity.

Publication Details

Journal
ArXiv.org
Published
2025-09-24
Primary Topic
Prenatal Screening and Diagnostics
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Thermal resilience of the ITER tungsten first wall to runaway electron impact

ArXiv.org
Prenatal Screening and Diagnostics
article

Thermal resilience of the ITER tungsten first wall to runaway electron impact

article en

Abstract

The fast volumetric deposition of multi-MeV high current runaway electron (RE) beams constitutes the most critical issue for the ITER tungsten (W) first wall (FW) longevity. Such relativistic electron beams could generate extreme volumetric power densities inside the FW armour which lead to significant vaporization, deep melting and even material explosions, as well as to elevated temperatures at the bond interface with the cooling substrate that could cause rupture and water leaks. Here the thermal response of the ITER FW is modeled with a three-stage, one-way coupled workflow focusing on assessments of the extent of the wall damage and the increase of the bond interface temperature for varying W thickness. Increased W thickness is found to be essential for wall protection against intense RE dissipation events in terms of both W tile damage and cooling system integrity.

ArXiv.org
Openalex Percentile: Top 31%
Prenatal Screening and Diagnostics
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Thermal resilience of the ITER tungsten first wall to runaway electron impact · ArXiv.org (2025) | TGRS Research Map | TGRS