Effect of annealing temperature on microstructure and properties of Ti 3Al-5Fe-1Cr titanium alloy golf club

Titanium alloy is a common material of golf clubs. Ti-3Al-1-5Fe-1Cr titanium alloy is a relatively successful golf club material because it enhances the anti-elasticity of golf clubs. The Ti-3Al-1,5Fe-1Cr dual phase titanium alloy was studied. The microstructure and mechanical properties of the alloy after annealing treatment were studied. The effects of annealing treatment on the microstructure, hardness, strength, plasticity and toughness of the alloy were clarified. After annealing treatment, the microstructure of the alloy is composed of cluster-like staggered lamellar α phase and β phase. When the annealing temperature is 850 °C, the hardness of the alloy is the highest 447 HV, the tensile strength is the highest 958 MPa, and the elongation after fracture is 16 %.

Institutions

Publication Details

Journal
SHILAP Revista de lepidopterología
Published
2025-01-01
Primary Topic
Titanium Alloys Microstructure and Properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Effect of annealing temperature on microstructure and properties of Ti 3Al-5Fe-1Cr titanium alloy golf club

SHILAP Revista de lepidopterología
Titanium Alloys Microstructure and Properties
article

Effect of annealing temperature on microstructure and properties of Ti 3Al-5Fe-1Cr titanium alloy golf club

article en

Abstract

Titanium alloy is a common material of golf clubs. Ti-3Al-1-5Fe-1Cr titanium alloy is a relatively successful golf club material because it enhances the anti-elasticity of golf clubs. The Ti-3Al-1,5Fe-1Cr dual phase titanium alloy was studied. The microstructure and mechanical properties of the alloy after annealing treatment were studied. The effects of annealing treatment on the microstructure, hardness, strength, plasticity and toughness of the alloy were clarified. After annealing treatment, the microstructure of the alloy is composed of cluster-like staggered lamellar α phase and β phase. When the annealing temperature is 850 °C, the hardness of the alloy is the highest 447 HV, the tensile strength is the highest 958 MPa, and the elongation after fracture is 16 %.

SHILAP Revista de lepidopterología
Harbin University (CN), Changchun Normal University (CN), Udon Thani Rajabhat University (TH), Industrial Development Bureau (TW)
Openalex Percentile: Top 60%
Titanium Alloys Microstructure and Properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.