Recovery of non-ferrous metals from Allarechensk waste dump by low-temperature roasting pathway

\nProcessing of Allarechensk technogenic deposit (Murmansk region, Russia) by the low-temperature roasting method in mixture with ammonium sulfate was carried out in a laboratory scale. The ore was grinded to various size classes, mixed with ammonium sulfate and the mixture was roasted in a muffle furnace under a static air atmosphere, varying the roasting temperature from 300 to 500 °C, roasting duration from 60 to 300 minutes. The roasted mixture was leached in heated distilled water with constant stirring for 40 minutes. Using a particle size class of -40 microns, a raw material to reagent ratio of 1:7, after roasting at a temperature of 400 °C at the water leaching stage the metals recovery was: Ni 91.5%, Cu 94.8%. Copper was extracted from the pregnant solution by the method of cementation on iron, and nickel was extracted by adding brucite (Mg(OH)2) to the solution.\n

Publication Details

Journal
Springer Link (Chiba Institute of Technology)
Published
2024-11-20
DOI
https://doi.org/10.1051/e3sconf/202459205012/pdf
Primary Topic
Seed and Plant Biochemistry
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Recovery of non-ferrous metals from Allarechensk waste dump by low-temperature roasting pathway

Springer Link (Chiba Institute of Technology)
Seed and Plant Biochemistry
article

Recovery of non-ferrous metals from Allarechensk waste dump by low-temperature roasting pathway

article en

Abstract

\nProcessing of Allarechensk technogenic deposit (Murmansk region, Russia) by the low-temperature roasting method in mixture with ammonium sulfate was carried out in a laboratory scale. The ore was grinded to various size classes, mixed with ammonium sulfate and the mixture was roasted in a muffle furnace under a static air atmosphere, varying the roasting temperature from 300 to 500 °C, roasting duration from 60 to 300 minutes. The roasted mixture was leached in heated distilled water with constant stirring for 40 minutes. Using a particle size class of -40 microns, a raw material to reagent ratio of 1:7, after roasting at a temperature of 400 °C at the water leaching stage the metals recovery was: Ni 91.5%, Cu 94.8%. Copper was extracted from the pregnant solution by the method of cementation on iron, and nickel was extracted by adding brucite (Mg(OH)2) to the solution.\n

Springer Link (Chiba Institute of Technology)
Ural Branch, Russian Academy of Sciences, Russian Academy of Sciences
Clean water and sanitation
Openalex Percentile: Top 51%
Seed and Plant Biochemistry
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.