Utilizationof High-Silicon Iron Ore Tailings for4N8 High-Purity Quartz Powder Production via Two-Stage Acid Leaching

This study investigates the process mechanisms for preparing 4N8 high-purity quartz powder from high-silicon iron ore tailings. Silicon concentrate obtained by wet high-intensity magnetic separation was used as the raw material, with impurities removed through a two-stage acid leaching process. The effects of acid concentration, temperature, time, and liquid–solid ratio on impurity removal were examined. Thermodynamic analysis shows that HF enhances the dissolution of Fe and Al impurities. In the first stage, response surface optimization determined the optimal conditions: acid concentration of 11.69 mol/L, temperature of 99.5 °C, and reaction time of 6.3 h, yielding SiO<sub>2</sub> purity of 99.949%. Kinetic analysis indicates Fe leaching is controlled by a chemical reaction (activation energy: 66.69 kJ/mol), while Al leaching is limited by internal diffusion (activation energy: 13.64 kJ/mol). The second-stage leaching, conducted at 10 mol/L acid concentration, 250 °C, and a liquid–solid ratio of 5:1 for 9 h, further reduced impurities. The final 4N8 high-purity quartz powder was obtained through fine grinding and high-temperature treatment. These findings provide theoretical guidance for the high-value utilization of iron ore tailings in applications such as semiconductors and photovoltaics.

Publication Details

Journal
Figshare
Published
2025-02-20
DOI
https://doi.org/10.1021/acs.inorgchem.4c04882.s001
Primary Topic
Wheat and Barley Genetics and Pathology
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Utilizationof High-Silicon Iron Ore Tailings for4N8 High-Purity Quartz Powder Production via Two-Stage Acid Leaching

Figshare
Wheat and Barley Genetics and Pathology
article

Utilizationof High-Silicon Iron Ore Tailings for4N8 High-Purity Quartz Powder Production via Two-Stage Acid Leaching

article en

Abstract

This study investigates the process mechanisms for preparing 4N8 high-purity quartz powder from high-silicon iron ore tailings. Silicon concentrate obtained by wet high-intensity magnetic separation was used as the raw material, with impurities removed through a two-stage acid leaching process. The effects of acid concentration, temperature, time, and liquid–solid ratio on impurity removal were examined. Thermodynamic analysis shows that HF enhances the dissolution of Fe and Al impurities. In the first stage, response surface optimization determined the optimal conditions: acid concentration of 11.69 mol/L, temperature of 99.5 °C, and reaction time of 6.3 h, yielding SiO<sub>2</sub> purity of 99.949%. Kinetic analysis indicates Fe leaching is controlled by a chemical reaction (activation energy: 66.69 kJ/mol), while Al leaching is limited by internal diffusion (activation energy: 13.64 kJ/mol). The second-stage leaching, conducted at 10 mol/L acid concentration, 250 °C, and a liquid–solid ratio of 5:1 for 9 h, further reduced impurities. The final 4N8 high-purity quartz powder was obtained through fine grinding and high-temperature treatment. These findings provide theoretical guidance for the high-value utilization of iron ore tailings in applications such as semiconductors and photovoltaics.

Figshare
Openalex Percentile: Top 41%
Wheat and Barley Genetics and Pathology
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.