Release coating for obtaining sand‑resin rods manufactured using heated tools

The article presents the results of research on the development of the lubricant composition for the production of sand‑resin rods over a heated tooling with high technological and consumer properties. It has been established that the conditional viscosity of the developed lubricant compositions decreases when oleic acid is added to the polymethylsiloxane liquid in an amount of 5 to 25 % from 10 to 8 s, and the density of lubricants is reduced from 908 to 882 kg/m3. It has been established that when oleic acid is added to the base in an amount of 15 %, the sedimentation stability of the lubricant is increased by more than 30 times. It is shown that the developed lubricant composition has the best lubrication characteristics at the following component ratio: base (polymethylsiloxane liquid PMS 300) 15 %, additive (oleic acid) 15 %, surfactant 3,0 %, water – the rest. The results of the research can be used by the process engineers when choosing the composition of the lubricant for making rods by the heated tooling.

Institutions

Publication Details

Journal
Litiyo i Metallurgiya (FOUNDRY PRODUCTION AND METALLURGY)
Published
2025-06-17
DOI
https://doi.org/10.21122/1683-6065-2025-2-46-51
Primary Topic
Materials Engineering and Processing
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Release coating for obtaining sand‑resin rods manufactured using heated tools

Litiyo i Metallurgiya (FOUNDRY PRODUCTION AND METALLURGY)
Materials Engineering and Processing
article

Release coating for obtaining sand‑resin rods manufactured using heated tools

article en

Abstract

The article presents the results of research on the development of the lubricant composition for the production of sand‑resin rods over a heated tooling with high technological and consumer properties. It has been established that the conditional viscosity of the developed lubricant compositions decreases when oleic acid is added to the polymethylsiloxane liquid in an amount of 5 to 25 % from 10 to 8 s, and the density of lubricants is reduced from 908 to 882 kg/m3. It has been established that when oleic acid is added to the base in an amount of 15 %, the sedimentation stability of the lubricant is increased by more than 30 times. It is shown that the developed lubricant composition has the best lubrication characteristics at the following component ratio: base (polymethylsiloxane liquid PMS 300) 15 %, additive (oleic acid) 15 %, surfactant 3,0 %, water – the rest. The results of the research can be used by the process engineers when choosing the composition of the lubricant for making rods by the heated tooling.

Litiyo i Metallurgiya (FOUNDRY PRODUCTION AND METALLURGY)(2)
Yanka Kupala State University of Grodno (BY)
Openalex Percentile: Top 55%
Materials Engineering and Processing
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.