Long-term development of mechanical properties of concrete with different water to cement ratio and internal curing ability

Concretes with water to cement (or binder) ratios of 0.50. 0.40, 0.30 and 0.20 were prepared and long-term mechanical properties were measured. Porous light-weight aggregates (LWA) in dosages of 10 % and 20 % were used for self-curing (internal curing) as a partial replacement of fine aggregates for some concrete types. Two environmental conditions were studied i.e., one under water and the other in foil, which prevents the extensive water exchange with the environment. Measured strengths at the ages of 28, 91, 365 and 720 days show higher values for the specimens covered in foil than for the specimens stored in water. On the other hand, the presence of LWAs reduces the compressive strength and bending strength of concrete with w/c = 0.30 at the age of 28 days of curing. The tests performed at the ages of 91 days and 1 year show higher flexural strengths than those of specimens cured in foil than those cured in water and those with internal curing.

Institutions

Publication Details

Journal
Zenodo (CERN European Organization for Nuclear Research)
Published
2024-11-28
DOI
https://doi.org/10.5281/zenodo.15275538
Primary Topic
Heat and Mass Transfer in Porous Media
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Long-term development of mechanical properties of concrete with different water to cement ratio and internal curing ability

Zenodo (CERN European Organization for Nuclear Research)
Heat and Mass Transfer in Porous Media
article

Long-term development of mechanical properties of concrete with different water to cement ratio and internal curing ability

article en

Abstract

Concretes with water to cement (or binder) ratios of 0.50. 0.40, 0.30 and 0.20 were prepared and long-term mechanical properties were measured. Porous light-weight aggregates (LWA) in dosages of 10 % and 20 % were used for self-curing (internal curing) as a partial replacement of fine aggregates for some concrete types. Two environmental conditions were studied i.e., one under water and the other in foil, which prevents the extensive water exchange with the environment. Measured strengths at the ages of 28, 91, 365 and 720 days show higher values for the specimens covered in foil than for the specimens stored in water. On the other hand, the presence of LWAs reduces the compressive strength and bending strength of concrete with w/c = 0.30 at the age of 28 days of curing. The tests performed at the ages of 91 days and 1 year show higher flexural strengths than those of specimens cured in foil than those cured in water and those with internal curing.

Zenodo (CERN European Organization for Nuclear Research)
VSB - Technical University of Ostrava (CZ), Czech Academy of Sciences, Institute of Physics of Materials (CZ), Brno University of Technology (CZ)
Clean water and sanitation
Openalex Percentile: Top 61%
Heat and Mass Transfer in Porous Media
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.