Study on the Solidification/Stabilizationof MSWIFly Ash by Composite Alkali-Activated Cementitious Materials

Municipal solid waste incineration (MSWI) fly ash (FA) is a hazardous waste produced during the incineration of municipal solid waste, posing a risk of heavy metal leaching and threatening the environment. Therefore, the harmless treatment of MSWI FA has become a crucial issue in environmental safety treatment. This study utilized blast furnace slag, FA, and MSWI FA to prepare composite alkali-activated cementitious materials for the solidification and stabilization of heavy metals in MSWI FA. The results showed that when the MSWI FA content was 30%, the water glass modulus was 1.0, the liquid–solid ratio was 0.32, the initial 24 h curing temperature was 45 °C, and the compressive strength of the solidified body reached 41.9 MPa, demonstrating excellent mechanical properties. Additionally, the leaching concentration and nonresidual state of heavy metals (Pb, Cd, and Cu) reduced significantly. Along with XRD, FTIR, and SEM-EDS analyses, it was revealed that the immobilization mechanism of heavy metals in the solidified body primarily involved physical encapsulation and chemical bonding.

Publication Details

Journal
Figshare
Published
2025-02-04
DOI
https://doi.org/10.1021/acsomega.4c08962.s001
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Study on the Solidification/Stabilizationof MSWIFly Ash by Composite Alkali-Activated Cementitious Materials

Figshare
Concrete and Cement Materials Research
article

Study on the Solidification/Stabilizationof MSWIFly Ash by Composite Alkali-Activated Cementitious Materials

article en

Abstract

Municipal solid waste incineration (MSWI) fly ash (FA) is a hazardous waste produced during the incineration of municipal solid waste, posing a risk of heavy metal leaching and threatening the environment. Therefore, the harmless treatment of MSWI FA has become a crucial issue in environmental safety treatment. This study utilized blast furnace slag, FA, and MSWI FA to prepare composite alkali-activated cementitious materials for the solidification and stabilization of heavy metals in MSWI FA. The results showed that when the MSWI FA content was 30%, the water glass modulus was 1.0, the liquid–solid ratio was 0.32, the initial 24 h curing temperature was 45 °C, and the compressive strength of the solidified body reached 41.9 MPa, demonstrating excellent mechanical properties. Additionally, the leaching concentration and nonresidual state of heavy metals (Pb, Cd, and Cu) reduced significantly. Along with XRD, FTIR, and SEM-EDS analyses, it was revealed that the immobilization mechanism of heavy metals in the solidified body primarily involved physical encapsulation and chemical bonding.

Figshare
Openalex Percentile: Top 55%
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.