Liquid-PhaseFurfural Hydrogenation over Ni/AluminaCatalysts

Furfural is an important platform chemical for producing value-added biobased molecules and materials as alternatives to fossil-derived chemical building blocks. Furfuryl alcohol (FALC) is one such valuable product, whose sustainable synthesis requires the catalytic reduction of furfural over Earth-abundant elements under mild conditions. Here, we report the liquid-phase hydrogenation of furfural over Ni nanoparticles prepared by either wet impregnation of alumina or exsolution from a NiAl layered double hydroxide (LDH). Exsolved and calcined Ni nanoparticles (NPs) spanned 11–18 nm, whereas the wet impregnation of [γ+δ]Al<sub>2</sub>O<sub>3</sub> yielded large Ni particles (24–101 nm) indicative of weak metal–support interactions. All catalysts exhibited moderate acid loadings (0.3–0.9 mmol·g<sup>–1</sup>) and weak basicity. Furfural conversion at 10 bar H<sub>2</sub> and 165 °C is inversely proportional to Ni particle size and structure-insensitive. Ni metal is the active site for furfural hydrogenation to FALC (specific activity of 84 mmol.g<sub>(Ni)</sub><sup>–1</sup>·h<sup>–1</sup> for NiAl-LDH, six times faster than Al<sub>2</sub>O<sub>3</sub>-supported Ni analogues with similar loading, and superior to many precious metal catalysts). FALC was the primary product at isoconversion with 60% selectivity but prone to secondary reactions at high furfural conversion, notably hydrogenolysis to 2-methylfuran (2-MF) or ring hydrogenation to tetrahydrofuryl alcohol (THFA). THFA was itself susceptible to hydrodeoxygenation over small Ni NPs at 10 bar H<sub>2</sub> in the presence of an acidic support to form 2-methyltetrahydrofuran (2-MTHF) via a previously unreported pathway. Higher hydrogen pressures favored FALC ring hydrogenation to THFA. Furfural hydrogenation to FALC was structure-insensitive for Ni NPs spanning 11–101 nm; however, secondary reactions of FALC were structure-sensitive. LDH-derived catalysts with 11 nm Ni NPs achieved a high yield of 2-MTHF (73%), a green solvent, liquid electrolyte, and high-density fuel additive. Furfural inhibited ring hydrogenation of reactively formed FALC (versus its hydrogenolysis or HDO), suppressing THFA and 2-MTHF production. However, ring hydrogenation of reactively formed FALC is favored at 25 bar H<sub>2</sub>, albeit with THFA, the dominant product.

Publication Details

Journal
Figshare
Published
2025-02-13
DOI
https://doi.org/10.1021/acssuschemeng.4c09477.s001
Primary Topic
Catalysis for Biomass Conversion
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Liquid-PhaseFurfural Hydrogenation over Ni/AluminaCatalysts

Figshare
Catalysis for Biomass Conversion
article

Liquid-PhaseFurfural Hydrogenation over Ni/AluminaCatalysts

article en

Abstract

Furfural is an important platform chemical for producing value-added biobased molecules and materials as alternatives to fossil-derived chemical building blocks. Furfuryl alcohol (FALC) is one such valuable product, whose sustainable synthesis requires the catalytic reduction of furfural over Earth-abundant elements under mild conditions. Here, we report the liquid-phase hydrogenation of furfural over Ni nanoparticles prepared by either wet impregnation of alumina or exsolution from a NiAl layered double hydroxide (LDH). Exsolved and calcined Ni nanoparticles (NPs) spanned 11–18 nm, whereas the wet impregnation of [γ+δ]Al<sub>2</sub>O<sub>3</sub> yielded large Ni particles (24–101 nm) indicative of weak metal–support interactions. All catalysts exhibited moderate acid loadings (0.3–0.9 mmol·g<sup>–1</sup>) and weak basicity. Furfural conversion at 10 bar H<sub>2</sub> and 165 °C is inversely proportional to Ni particle size and structure-insensitive. Ni metal is the active site for furfural hydrogenation to FALC (specific activity of 84 mmol.g<sub>(Ni)</sub><sup>–1</sup>·h<sup>–1</sup> for NiAl-LDH, six times faster than Al<sub>2</sub>O<sub>3</sub>-supported Ni analogues with similar loading, and superior to many precious metal catalysts). FALC was the primary product at isoconversion with 60% selectivity but prone to secondary reactions at high furfural conversion, notably hydrogenolysis to 2-methylfuran (2-MF) or ring hydrogenation to tetrahydrofuryl alcohol (THFA). THFA was itself susceptible to hydrodeoxygenation over small Ni NPs at 10 bar H<sub>2</sub> in the presence of an acidic support to form 2-methyltetrahydrofuran (2-MTHF) via a previously unreported pathway. Higher hydrogen pressures favored FALC ring hydrogenation to THFA. Furfural hydrogenation to FALC was structure-insensitive for Ni NPs spanning 11–101 nm; however, secondary reactions of FALC were structure-sensitive. LDH-derived catalysts with 11 nm Ni NPs achieved a high yield of 2-MTHF (73%), a green solvent, liquid electrolyte, and high-density fuel additive. Furfural inhibited ring hydrogenation of reactively formed FALC (versus its hydrogenolysis or HDO), suppressing THFA and 2-MTHF production. However, ring hydrogenation of reactively formed FALC is favored at 25 bar H<sub>2</sub>, albeit with THFA, the dominant product.

Figshare
Responsible consumption and production
Openalex Percentile: Top 58%
Catalysis for Biomass Conversion
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.