Integrated micro and nano-silica in advanced composite high-strength mortar for TRM system

This study presents the development of a high-strength composite mortar for Textile Reinforced Mortar (TRM) systems through the synergistic integration of micro-silica, nano-silica, silica sand, and hybrid fibers. The combination of steel and basalt fibers significantly enhanced the mechanical and bonding performance of the mortar. The optimized mix achieved compressive, split tensile, and flexural strengths of 70.335 MPa, 8.03 MPa, and 19.63 MPa, respectively, while demonstrating improved bonding behavior with an 80.5% increase in splitting bond strength, direct pull-off bond strength of 8.5 MPa, and pull-out bond strength of 7.0 MPa. These improvements are attributed to the densified microstructure and refined interfacial transition zone resulting from the pozzolanic reactions of micro- and nano-silica. The findings confirm that the combined use of multi-scale silica materials and hybrid fibers produces superior mechanical strength, durability, and adhesion, making the developed mortar a promising solution for retrofitting and strengthening applications in modern construction.

Authors

Institutions

Publication Details

Journal
Scientific Reports
Published
2025-11-27
DOI
https://doi.org/10.1038/s41598-025-25513-3
Primary Topic
Masonry and Concrete Structural Analysis
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Integrated micro and nano-silica in advanced composite high-strength mortar for TRM system

Manisha Shewale, R. Siva Chidambaram, Bhagyashree Khartode, R. Gobinath et al.
Scientific Reports
Masonry and Concrete Structural Analysis
article

Integrated micro and nano-silica in advanced composite high-strength mortar for TRM system

Manisha Shewale, R. Siva Chidambaram, Bhagyashree Khartode, R. Gobinath, Nitin Shinde
article en

Abstract

This study presents the development of a high-strength composite mortar for Textile Reinforced Mortar (TRM) systems through the synergistic integration of micro-silica, nano-silica, silica sand, and hybrid fibers. The combination of steel and basalt fibers significantly enhanced the mechanical and bonding performance of the mortar. The optimized mix achieved compressive, split tensile, and flexural strengths of 70.335 MPa, 8.03 MPa, and 19.63 MPa, respectively, while demonstrating improved bonding behavior with an 80.5% increase in splitting bond strength, direct pull-off bond strength of 8.5 MPa, and pull-out bond strength of 7.0 MPa. These improvements are attributed to the densified microstructure and refined interfacial transition zone resulting from the pozzolanic reactions of micro- and nano-silica. The findings confirm that the combined use of multi-scale silica materials and hybrid fibers produces superior mechanical strength, durability, and adhesion, making the developed mortar a promising solution for retrofitting and strengthening applications in modern construction.

Scientific ReportsVol. 15(1)
Symbiosis International University (IN), Central Building Research Institute (IN)
Openalex Percentile: Top 62%
Masonry and Concrete Structural Analysis
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Integrated micro and nano-silica in advanced composite high-strength mortar for TRM system — Manisha Shewale, R. Siva Chidambaram, et al. · Scientific Reports (2025) | TGRS Research Map | TGRS