Adsorption Mechanism of SF <sub>6</sub> Decomposed Toxic Gases (H <sub>2</sub> S, SO <sub>2</sub> , SO <sub>2</sub> F <sub>2</sub> ) on Pt-Modified Janus SnSSe Monolayer: A Density Functional Theory Study

This study explores the sensing capabilities of Pt-decorated Janus SnSSe monolayers toward SF<sub>6</sub> decomposition gases (H<sub>2</sub>S, SO<sub>2</sub>, and SO<sub>2</sub>F<sub>2</sub>) using density functional theory (DFT). Findings reveal that the introduction of Pt atoms onto either the S- or Se-terminated surface of the SnSSe monolayer markedly improves both the adsorption strength and structural integrity of the material. Adsorption behavior and underlying sensing mechanisms across different gas-substrate systems were comprehensively investigated by examining adsorption energy, adsorption distance, charge density, density of states, orbital interaction, recovery time, sensitivity, and work function. The results indicate that the pristine SnSSe monolayer exhibits only physical adsorption and is unsuitable for detecting any of the three target gases. In contrast, Pt-modified SnSSe demonstrates significantly enhanced gas adsorption. On the S-surface, adsorption energies for H<sub>2</sub>S, SO<sub>2</sub>, and SO<sub>2</sub>F<sub>2</sub> were -0.981 eV, -0.751 eV, and -0.026 eV, respectively, while on the Se-surface, the values were -0.954 eV, -0.776 eV, and -0.026 eV. At the optimal operating temperature, the recovery time for the Pt-SnSSe(S)/H<sub>2</sub>S system is 64.67 s, while the recovery times for Pt-SnSSe(Se) toward H<sub>2</sub>S and SO<sub>2</sub> are 26.75 and 13.02 s, respectively. Both modified surfaces exhibited poor adsorption performance toward SO<sub>2</sub>F<sub>2</sub>. This study offers theoretical insights for designing low-power, high-sensitivity, and fast-response gas sensors used to detect SF<sub>6</sub> decomposition products in gas-insulated switchgear (GIS).

Authors

Institutions

Publication Details

Journal
Langmuir
Published
2025-11-20
DOI
https://doi.org/10.1021/acs.langmuir.5c04640
Primary Topic
2D Materials and Applications
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Adsorption Mechanism of SF 6 Decomposed Toxic Gases (H 2 S, SO 2 , SO 2 F 2 ) on Pt-Modified Janus SnSSe Monolayer: A Density Functional Theory Study

Runtong Zhu, Y. N. Gao
Langmuir
2D Materials and Applications
article

Adsorption Mechanism of SF 6 Decomposed Toxic Gases (H 2 S, SO 2 , SO 2 F 2 ) on Pt-Modified Janus SnSSe Monolayer: A Density Functional Theory Study

Runtong Zhu, Y. N. Gao
article en

Abstract

This study explores the sensing capabilities of Pt-decorated Janus SnSSe monolayers toward SF<sub>6</sub> decomposition gases (H<sub>2</sub>S, SO<sub>2</sub>, and SO<sub>2</sub>F<sub>2</sub>) using density functional theory (DFT). Findings reveal that the introduction of Pt atoms onto either the S- or Se-terminated surface of the SnSSe monolayer markedly improves both the adsorption strength and structural integrity of the material. Adsorption behavior and underlying sensing mechanisms across different gas-substrate systems were comprehensively investigated by examining adsorption energy, adsorption distance, charge density, density of states, orbital interaction, recovery time, sensitivity, and work function. The results indicate that the pristine SnSSe monolayer exhibits only physical adsorption and is unsuitable for detecting any of the three target gases. In contrast, Pt-modified SnSSe demonstrates significantly enhanced gas adsorption. On the S-surface, adsorption energies for H<sub>2</sub>S, SO<sub>2</sub>, and SO<sub>2</sub>F<sub>2</sub> were -0.981 eV, -0.751 eV, and -0.026 eV, respectively, while on the Se-surface, the values were -0.954 eV, -0.776 eV, and -0.026 eV. At the optimal operating temperature, the recovery time for the Pt-SnSSe(S)/H<sub>2</sub>S system is 64.67 s, while the recovery times for Pt-SnSSe(Se) toward H<sub>2</sub>S and SO<sub>2</sub> are 26.75 and 13.02 s, respectively. Both modified surfaces exhibited poor adsorption performance toward SO<sub>2</sub>F<sub>2</sub>. This study offers theoretical insights for designing low-power, high-sensitivity, and fast-response gas sensors used to detect SF<sub>6</sub> decomposition products in gas-insulated switchgear (GIS).

LangmuirVol. 41(48)
Shanghai Tunnel Engineering Rail Transit Design & Research Institute (CN), Shanghai Institute of Technology (CN)
Openalex Percentile: Top 71%
2D Materials and Applications
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.