Monitoring the effect of runout on a Diamond-Coated Burrs’ wear progression with Acoustic Emission

Recent Tool Condition Monitoring (TCM) approaches aim to optimise tool replacement by reducing unutilised Remaining Useful Life (RUL) and preventing unexpected failures of Diamond-Coated Burrs (DCBs). Acoustic Emission (AE) has been established as an indirect monitoring method for DCB wear through precision tool measurements. This study assesses the impact of changing initial runout on both wear progression and AE-based monitoring. Twelve wear tests were conducted using an adjustable tool-holder to vary initial runout between 1–78 µm, with AE and frequent on-machine surface measurements collected throughout. Results show that increased initial runout negatively affects total tool life and introduces greater variability in wear behaviour under identical conditions. Using a Renishaw NC4+ Blue (NC4) system, a high frequency of measurements enabled tracking of each DCB’s progression through the three wear phases. Surface crater formation and circumferential wear band expansion were consistently observed in the final wear phase of all DCBs. AE proved effective in monitoring both runout severity and the wear progression of the tool’s high spot. AE features also identified key wear points throughout the tool’s life, regardless of initial runout. These findings highlight the critical influence of runout on small-diameter DCB performance and support AE as a reliable, indirect, on-machine sensing method for tool wear monitoring, capable of identifying varying initial tool conditions. • Effect of runout on diamond-coated burr wear using novel tool measurements. • Correlation of acoustic emission generated during grinding to tool wear mechanisms. • Validation of acoustic emission for tool condition monitoring.

Authors

Institutions

Publication Details

Journal
Wear
Published
2025-11-21
DOI
https://doi.org/10.1016/j.wear.2025.206420
Primary Topic
Advanced machining processes and optimization
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Monitoring the effect of runout on a Diamond-Coated Burrs’ wear progression with Acoustic Emission

Rhys Pullin, Mark Eaton, Thomas Jessel, Ben Merrifield et al.
Wear
Advanced machining processes and optimization
article

Monitoring the effect of runout on a Diamond-Coated Burrs’ wear progression with Acoustic Emission

Rhys Pullin, Mark Eaton, Thomas Jessel, Ben Merrifield, Carl Byrne
article en

Abstract

Recent Tool Condition Monitoring (TCM) approaches aim to optimise tool replacement by reducing unutilised Remaining Useful Life (RUL) and preventing unexpected failures of Diamond-Coated Burrs (DCBs). Acoustic Emission (AE) has been established as an indirect monitoring method for DCB wear through precision tool measurements. This study assesses the impact of changing initial runout on both wear progression and AE-based monitoring. Twelve wear tests were conducted using an adjustable tool-holder to vary initial runout between 1–78 µm, with AE and frequent on-machine surface measurements collected throughout. Results show that increased initial runout negatively affects total tool life and introduces greater variability in wear behaviour under identical conditions. Using a Renishaw NC4+ Blue (NC4) system, a high frequency of measurements enabled tracking of each DCB’s progression through the three wear phases. Surface crater formation and circumferential wear band expansion were consistently observed in the final wear phase of all DCBs. AE proved effective in monitoring both runout severity and the wear progression of the tool’s high spot. AE features also identified key wear points throughout the tool’s life, regardless of initial runout. These findings highlight the critical influence of runout on small-diameter DCB performance and support AE as a reliable, indirect, on-machine sensing method for tool wear monitoring, capable of identifying varying initial tool conditions. • Effect of runout on diamond-coated burr wear using novel tool measurements. • Correlation of acoustic emission generated during grinding to tool wear mechanisms. • Validation of acoustic emission for tool condition monitoring.

WearVol. 584-585
Renishaw (United Kingdom) (GB), Cardiff University (GB)
Openalex Percentile: Top 63%
Advanced machining processes and optimization
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Monitoring the effect of runout on a Diamond-Coated Burrs’ wear progression with Acoustic Emission — Rhys Pullin, Mark Eaton, et al. · Wear (2025) | TGRS Research Map | TGRS