Effect of polishing sequence on the surface roughness and flexural strength of additively or subtractively manufactured zirconia
Polishing performed both before and after sintering enabled clinically acceptable surface roughness for AM zirconia. In all polished specimens, AM specimens polished before and after sintering had the highest flexural strength.
Authors
- Abdulaziz Alhotan (ORCID: https://orcid.org/0000-0002-9036-0485)
- Manrique Fonseca (ORCID: https://orcid.org/0000-0003-4267-0515)
- Selin Çelik Öge (ORCID: https://orcid.org/0000-0003-1403-6832)
- Burak Yılmaz (ORCID: https://orcid.org/0000-0002-7101-363X)
- Gülce Çakmak (ORCID: https://orcid.org/0000-0003-1751-9207)
- Damla Erkal (ORCID: https://orcid.org/0000-0001-8319-6974)
Institutions
- University of Bern (CH)
- Ankara University (TR)
- King Saud University (SA)
- Humboldt-Universität zu Berlin (DE)
- The Ohio State University (US)
- Burdur Mehmet Akif Ersoy Üniversitesi (TR)
- Cukurova University (TR)
Publication Details
- Journal
- Journal of Prosthodontics
- Published
- 2025-11-21
- DOI
- https://doi.org/10.1111/jopr.70061
- Primary Topic
- Dental materials and restorations
- Type
- article
- Field-Weighted Citation Impact
- 0.00