Regeneration of battery grade FePO4 and Li2CO3 from Al/F-bearing spent LiFePO4/C powder
A sustainable approach for recovering battery grade FePO 4 and Li 2 CO 3 from Al/F-bearing spent LiFePO 4 /C powder was proposed, including acid leaching, fluorinated coordination precipitation, homogeneous precipitation, and high-temperature precipitation. Under the optimal conditions, the leaching efficiencies of Li, Fe, P, Al, and F were 97.6%, 97.1%, 97.1%, 72.5%, and 63.3%, respectively. The effects of different parameters on the removal of Al/F impurities were systematically evaluated, indicating about 99.4% Al and 96.4% F in the leachate were precipitated in the form of Na 3 Li 3 Al 2 F 12 , and their residual concentrations were only 0.0124 and 0.328 g/L, respectively, which could be directly used to prepare battery grade FePO 4 (99.68% in purity). Lithium in the Al/F-bearing residue could be extracted through CaCO 3 -CaSO 4 roasting followed by acid leaching, ultimately obtaining 99.87% purity of Li 2 CO 3 . The recovery rates of Li and Fe were 96.88% and 92.85%, respectively. An economic evaluation demonstrated that the process was profitable.
Authors
- Kanggen Zhou
- Changhong Peng (ORCID: https://orcid.org/0000-0003-0368-9301)
- Kai Zhang (ORCID: https://orcid.org/0000-0002-3830-9682)
- Wei Chen (ORCID: https://orcid.org/0000-0002-1131-3585)
- Kui Yi (ORCID: https://orcid.org/0000-0003-3585-1852)
- Jing-kun DENG
- Zeyang Qiu (ORCID: https://orcid.org/0009-0002-7007-1448)
- Yehuizi Wu
Institutions
- Central South University (CN)
Publication Details
- Journal
- Transactions of Nonferrous Metals Society of China
- Published
- 2025-10-01
- DOI
- https://doi.org/10.1016/s1003-6326(25)66897-x
- Citations
- 1
- Primary Topic
- Extraction and Separation Processes
- Type
- article
- Field-Weighted Citation Impact
- 0.71