Monitoring Depolymerization in Mesopores Using Dynamic Properties of Polymeric Melt Accessed via Dielectric Spectroscopy

Traditional design principles for heterogeneous catalysis guide the use of catalytic particles with mesosized (∼2–50 nm) pores to increase the number of surface-active sites by way of an increased surface area. However, the entry of long-chain polymers into such pores may be significantly limited by the size and entanglement of polymers in the melt state, thereby decreasing the number of accessible sites. Assessment of catalyst performance from traditional reactor-based studies averages over intrapore reaction events as well as reactions on the surface of a particle, resulting in an inability to distinguish between differences in site accessibility and activity. Techniques that assess the intrapore performance can inform the design of future heterogeneous catalysts for polymer upcycling. In this work, we demonstrate the use of broadband dielectric spectroscopy to monitor depolymerization of a polymer melt within mesopores via changes in the segmental relaxation time scale of amorphous polymer chains. In particular, we highlight the use of an anodic aluminum oxide (AAO) membrane as a readily available model for catalyst pores with a well-characterized pore morphology. The decrease in the segmental relaxation (α-relaxation) time of the melt with increasing chain scission emerges as a measure of the extent of polymer deconstruction inside mesopores. To demonstrate the utility of this technique, we demonstrate the decomposition of two commercial poly(propylene carbonate) polymers with different decomposition rates within mesopores. As the polymers depolymerize, their segmental relaxation time decreases as the molecular weight decreases (as predicted by the Fox–Flory equation). The BDS-measured change in segmental relaxation time mirrors the expected trend based on change in molecular weight measured by size exclusion chromatography.

Authors

Institutions

Publication Details

Journal
Macromolecules
Published
2025-10-17
DOI
https://doi.org/10.1021/acs.macromol.5c01457
Primary Topic
Conducting polymers and applications
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Monitoring Depolymerization in Mesopores Using Dynamic Properties of Polymeric Melt Accessed via Dielectric Spectroscopy

Rachel A. Segalman, R. Venkatesh, Susannah L. Scott, Lynn M. Walker et al.
Macromolecules
Conducting polymers and applications
article

Monitoring Depolymerization in Mesopores Using Dynamic Properties of Polymeric Melt Accessed via Dielectric Spectroscopy

Rachel A. Segalman, R. Venkatesh, Susannah L. Scott, Lynn M. Walker, Jon Bingaman
article en

Abstract

Traditional design principles for heterogeneous catalysis guide the use of catalytic particles with mesosized (∼2–50 nm) pores to increase the number of surface-active sites by way of an increased surface area. However, the entry of long-chain polymers into such pores may be significantly limited by the size and entanglement of polymers in the melt state, thereby decreasing the number of accessible sites. Assessment of catalyst performance from traditional reactor-based studies averages over intrapore reaction events as well as reactions on the surface of a particle, resulting in an inability to distinguish between differences in site accessibility and activity. Techniques that assess the intrapore performance can inform the design of future heterogeneous catalysts for polymer upcycling. In this work, we demonstrate the use of broadband dielectric spectroscopy to monitor depolymerization of a polymer melt within mesopores via changes in the segmental relaxation time scale of amorphous polymer chains. In particular, we highlight the use of an anodic aluminum oxide (AAO) membrane as a readily available model for catalyst pores with a well-characterized pore morphology. The decrease in the segmental relaxation (α-relaxation) time of the melt with increasing chain scission emerges as a measure of the extent of polymer deconstruction inside mesopores. To demonstrate the utility of this technique, we demonstrate the decomposition of two commercial poly(propylene carbonate) polymers with different decomposition rates within mesopores. As the polymers depolymerize, their segmental relaxation time decreases as the molecular weight decreases (as predicted by the Fox–Flory equation). The BDS-measured change in segmental relaxation time mirrors the expected trend based on change in molecular weight measured by size exclusion chromatography.

MacromoleculesVol. 58(20)
University of Minnesota System (US), University of California System (US)
Openalex Percentile: Top 74%
Conducting polymers and applications
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.