On the surface integrity resulting from laser powder bed fusion of Ti6Al4V: Improvements by cavitation abrasive surface finishing

As the manufacturing readiness level of laser powder bed fusion (L-PBF) advances, post-processing has become increasingly important for achieving net-shape components and to enhance surface texture and integrity. Apart from surface roughness, one concern is the unique morphology of printed surfaces with vertical, upskin, and downskin inclinations. In this study, we characterized the surface texture and integrity of L-PBF Ti6Al4V with respect to build orientation. In the as-built condition, the downskin surfaces possessed the highest roughness, the largest effective surface stress concentration(),Ktand the greatest presence of partially melted powder particles fused to the surface. Cavitation abrasive surface finishing (CASF) was adopted to improve surface quality, with consideration of the build orientation. The results indicated that CASF reduced roughness, lowered Kt posed by the surface texture, and introduced compressive residual stress regardless of the build orientation. Downskin surfaces were the most challenging to treat; they exhibited substantially greater Ktthan the other orientations after treatment (>2×) and lower compressive residual stress (50%). More extensive powder coverage of the downskin surfaces appears to shield the underlying substrate from abrasive attack and direct implosion of cavitation bubbles, which are central to the CASF treatment mechanism. The importance of orientation to the effectiveness of CASF treatment is discussed, as well as strategies to overcome this challenge. Overall, downskin surfaces require greater surface treatment intensity or duration to obtain the same degree of improvement.

Authors

Publication Details

Journal
Materials Science in Additive Manufacturing
Published
2025-10-14
DOI
https://doi.org/10.36922/msam025280062
Primary Topic
Additive Manufacturing Materials and Processes
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

On the surface integrity resulting from laser powder bed fusion of Ti6Al4V: Improvements by cavitation abrasive surface finishing

C. Wisdom, M. Ramulu, Alejandra Leonor Martínez, M Silvestre et al.
Materials Science in Additive Manufacturing
Additive Manufacturing Materials and Processes
article

On the surface integrity resulting from laser powder bed fusion of Ti6Al4V: Improvements by cavitation abrasive surface finishing

C. Wisdom, M. Ramulu, Alejandra Leonor Martínez, M Silvestre, A. Montelione, Dwayne Arola, Daniel G. Sanders, Cole Nouwens, Rohin Petram
article en

Abstract

As the manufacturing readiness level of laser powder bed fusion (L-PBF) advances, post-processing has become increasingly important for achieving net-shape components and to enhance surface texture and integrity. Apart from surface roughness, one concern is the unique morphology of printed surfaces with vertical, upskin, and downskin inclinations. In this study, we characterized the surface texture and integrity of L-PBF Ti6Al4V with respect to build orientation. In the as-built condition, the downskin surfaces possessed the highest roughness, the largest effective surface stress concentration(),Ktand the greatest presence of partially melted powder particles fused to the surface. Cavitation abrasive surface finishing (CASF) was adopted to improve surface quality, with consideration of the build orientation. The results indicated that CASF reduced roughness, lowered Kt posed by the surface texture, and introduced compressive residual stress regardless of the build orientation. Downskin surfaces were the most challenging to treat; they exhibited substantially greater Ktthan the other orientations after treatment (>2×) and lower compressive residual stress (50%). More extensive powder coverage of the downskin surfaces appears to shield the underlying substrate from abrasive attack and direct implosion of cavitation bubbles, which are central to the CASF treatment mechanism. The importance of orientation to the effectiveness of CASF treatment is discussed, as well as strategies to overcome this challenge. Overall, downskin surfaces require greater surface treatment intensity or duration to obtain the same degree of improvement.

Materials Science in Additive ManufacturingVol. 5(1)
Openalex Percentile: Top 70%
Additive Manufacturing Materials and Processes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

On the surface integrity resulting from laser powder bed fusion of Ti6Al4V: Improvements by cavitation abrasive surface finishing — C. Wisdom, M. Ramulu, et al. · Materials Science in Additive Manufacturing (2025) | TGRS Research Map | TGRS