In vitro study to assess shear bond strength of e-mineral trioxide aggregate with glass ionomer cement
The shear bond strength (SBS) between enhanced Mineral Trioxide Aggregate (e-MTA) and glass ionomer cement (GIC) under different placement intervals is of interest. Sixty acrylic blocks filled with e-MTA were restored with GIC at 0 min, 15 min and 24 h. The highest SBS (12.47 ± 1.29 MPa) was observed at the 15-minute interval. Predominantly mixed failures were seen in Groups II and III, while cohesive failures occurred in Group I. Applying GIC 15 minutes after e-MTA yields optimal bonding for durable restorations.
Authors
- Dhirendra Kumar Singh (ORCID: https://orcid.org/0000-0002-0457-9502)
- Ananya Bhargava (ORCID: https://orcid.org/0000-0002-9955-979X)
- Soumyaranjan Nanda
- Paramveer Singh (ORCID: https://orcid.org/0000-0002-4703-2646)
- Subasish Behera
- Anupama Ahirwar
- Apoorva Sharma (ORCID: https://orcid.org/0009-0001-9868-1662)
- Miral Mehta
Institutions
- Sant Gadge Baba Amravati University (IN)
- Sri Sri University (IN)
- Ruxmaniben Deepchand Gardi Medical College (IN)
- Government Medical College (IN)
- Government Dental College and Hospital (IN)
- Chhattisgarh Dental College & Research Institute (IN)
- People’s University (IN)
- National Law University Odisha (IN)
- Karnavati University
- KIIT University (IN)
Publication Details
- Journal
- Bioinformation
- Published
- 2025-09-30
- DOI
- https://doi.org/10.6026/973206300213301
- Primary Topic
- Endodontics and Root Canal Treatments
- Type
- article
- Field-Weighted Citation Impact
- 0.00