Reversal of Water Corrosion Behavior of Crystalline and Amorphous SiC with Increasing Temperature

The application of silicon carbide ceramic matrix composite (CMC-SiC) as hot-end components in next-generation advanced gas turbine is susceptible to corrosion by high-temperature, high-velocity water vapor present in combustion environments. Furthermore, its amorphous-crystalline composite structure results in a more complex corrosion response under water vapor exposure. Reactive molecular dynamics simulations were employed to investigate the differences in water corrosion behavior between crystalline and amorphous SiC over a temperature range of 1000-2000 K. At 1000 K, the amorphous SiC surface exhibits greater susceptibility due to its disordered atomic structure. In contrast, at 2000 K, the Si surface of 4H-SiC undergoes more severe corrosion. This reversal in corrosion behavior can be attributed to the formation and subsequent volatilization of the Si-O-Si network from the SiC slab. Specifically, the Si-O-Si network exhibits stronger bonding with the amorphous SiC surface, making it more resistant to corrosion by high-temperature water molecules. These findings offer valuable insights into the optimization of CMC-SiC hot-end components.

Authors

Institutions

Publication Details

Journal
Langmuir
Published
2025-10-02
DOI
https://doi.org/10.1021/acs.langmuir.5c03453
Primary Topic
Advanced ceramic materials synthesis
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Reversal of Water Corrosion Behavior of Crystalline and Amorphous SiC with Increasing Temperature

Pengfei Shi, Yang Wang, Lei Chen, Junting Li et al.
Langmuir
Advanced ceramic materials synthesis
article

Reversal of Water Corrosion Behavior of Crystalline and Amorphous SiC with Increasing Temperature

Pengfei Shi, Yang Wang, Lei Chen, Junting Li, Yexin Li, Linmao Qian
article en

Abstract

The application of silicon carbide ceramic matrix composite (CMC-SiC) as hot-end components in next-generation advanced gas turbine is susceptible to corrosion by high-temperature, high-velocity water vapor present in combustion environments. Furthermore, its amorphous-crystalline composite structure results in a more complex corrosion response under water vapor exposure. Reactive molecular dynamics simulations were employed to investigate the differences in water corrosion behavior between crystalline and amorphous SiC over a temperature range of 1000-2000 K. At 1000 K, the amorphous SiC surface exhibits greater susceptibility due to its disordered atomic structure. In contrast, at 2000 K, the Si surface of 4H-SiC undergoes more severe corrosion. This reversal in corrosion behavior can be attributed to the formation and subsequent volatilization of the Si-O-Si network from the SiC slab. Specifically, the Si-O-Si network exhibits stronger bonding with the amorphous SiC surface, making it more resistant to corrosion by high-temperature water molecules. These findings offer valuable insights into the optimization of CMC-SiC hot-end components.

LangmuirVol. 41(40)
Tribhuvan University (NP), Frontier Science Foundation (CH), Southwest Jiaotong University (CN), Chongqing Jiaotong University (CN)
Openalex Percentile: Top 76%
Advanced ceramic materials synthesis
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Reversal of Water Corrosion Behavior of Crystalline and Amorphous SiC with Increasing Temperature — Pengfei Shi, Yang Wang, et al. · Langmuir (2025) | TGRS Research Map | TGRS