The study of the formation of solid solutions of lithium in iridium

The interaction in the Li-Ir system using Li3N as a lithium source was studied depending on the temperature, heat treatment time and total pressure in the system. Using X-ray phase analysis (XRD), it was shown that heat treatment of a powder mixture of Li3N and Ir in a graphite or BN crucible in the temperature range of 800–1200°C leads to the formation of a substitution solid solution of Ir(Li), with the lithium content decreasing with increasing temperature, heat treatment time and decreasing total pressure in the system. The maximum lithium content in iridium reached 6.2% at. It was shown that the use of a closed BN container increases the yield of the Ir(Li) solid solution. The use of graphite or BN crucibles prevents the formation of intermetallic compounds of the Li-Ir system.

Authors

Publication Details

Journal
Журнал неорганической химии / Russian Journal of Inorganic Chemistry
Published
2025-01-01
DOI
https://doi.org/10.7868/s3034560x25060065
Primary Topic
Thermodynamic and Structural Properties of Metals and Alloys
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

The study of the formation of solid solutions of lithium in iridium

Victor V. Lozanov
Журнал неорганической химии / Russian Journal of Inorganic Chemistry
Thermodynamic and Structural Properties of Metals and Alloys
article

The study of the formation of solid solutions of lithium in iridium

Victor V. Lozanov
article en

Abstract

The interaction in the Li-Ir system using Li3N as a lithium source was studied depending on the temperature, heat treatment time and total pressure in the system. Using X-ray phase analysis (XRD), it was shown that heat treatment of a powder mixture of Li3N and Ir in a graphite or BN crucible in the temperature range of 800–1200°C leads to the formation of a substitution solid solution of Ir(Li), with the lithium content decreasing with increasing temperature, heat treatment time and decreasing total pressure in the system. The maximum lithium content in iridium reached 6.2% at. It was shown that the use of a closed BN container increases the yield of the Ir(Li) solid solution. The use of graphite or BN crucibles prevents the formation of intermetallic compounds of the Li-Ir system.

Журнал неорганической химии / Russian Journal of Inorganic ChemistryVol. 70(6)
Openalex Percentile: Top 72%
Thermodynamic and Structural Properties of Metals and Alloys
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.