Uji Durabilitas Beton Normal Setelah Perendaman dalam Air Laut dan Pembakaran pada Suhu Tinggi

This study aims to test the durability of normal concrete after exposure to a combination of two extreme conditions: immersion in seawater and burning at high temperatures (300°C, 400°C, and 500°C). The study is motivated by the vulnerability of structures in coastal areas to both aggressive chloride attacks and fire hazards. The concrete used was designed for 25 MPa compressive strength and tested at 28 days of age. Cylindrical specimens (15 cm diameter and 30 cm height) were immersed in seawater for 28 days, then burned in a drum furnace for 30 minutes at the specified temperatures. Testing included compressive strength, density, and porosity measurements. Results show significant deterioration at 500°C, moderate deterioration at 400°C, and minor deterioration at 300°C. This confirms the need for better durability strategies for concrete in extreme environments.

Authors

Institutions

Publication Details

Journal
Jurnal Proyek Teknik Sipil
Published
2025-09-29
DOI
https://doi.org/10.14710/potensi.2025.27672
Primary Topic
Geotechnical and construction materials studies
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Uji Durabilitas Beton Normal Setelah Perendaman dalam Air Laut dan Pembakaran pada Suhu Tinggi

Sandika Arjuna
Jurnal Proyek Teknik Sipil
Geotechnical and construction materials studies
article

Uji Durabilitas Beton Normal Setelah Perendaman dalam Air Laut dan Pembakaran pada Suhu Tinggi

Sandika Arjuna
article en

Abstract

This study aims to test the durability of normal concrete after exposure to a combination of two extreme conditions: immersion in seawater and burning at high temperatures (300°C, 400°C, and 500°C). The study is motivated by the vulnerability of structures in coastal areas to both aggressive chloride attacks and fire hazards. The concrete used was designed for 25 MPa compressive strength and tested at 28 days of age. Cylindrical specimens (15 cm diameter and 30 cm height) were immersed in seawater for 28 days, then burned in a drum furnace for 30 minutes at the specified temperatures. Testing included compressive strength, density, and porosity measurements. Results show significant deterioration at 500°C, moderate deterioration at 400°C, and minor deterioration at 300°C. This confirms the need for better durability strategies for concrete in extreme environments.

Jurnal Proyek Teknik SipilVol. 8(2)
Universitas Prof. Dr. Hazairin SH. (ID), University of Bengkulu (ID)
Openalex Percentile: Top 72%
Geotechnical and construction materials studies
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.