CO₂ Seeding Admixtures for Enhanced Concrete Activation

In this study, on-site CO2 seeding admixtures were prepared using power ultrasound-assisted pre-carbonation and chelator-assisted pre-carbonation (GLTA, EDTA) to enhance the carbonation efficiency and mechanical properties. Studies have shown that the application of power ultrasound can achieve a maximum CO2 uptake of 9.0% of the binder during the preacarbontion process. Compared with those of the traditional mixing batch and ordinary carbonation seeding activated batch, the strength of the power ultrasound seeding activated batch increased by 27.2 % and 21.4 %, respectively, after 1 day. Additionally, the EDTA-assisted pre-carbonation can achieve a maximum CO2 uptake of 9.6% of the binder during the preacarbontion process. Both early and later age strengths of cement mortar were enhanced by 21.33% at 1 day, 19.16% at 3 days, 16.00% at 7 days, and 16.38% at 28 days.

Authors

Publication Details

Published
2025-09-27
DOI
https://doi.org/10.5703/1288284318015
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

CO₂ Seeding Admixtures for Enhanced Concrete Activation

Guangqi Xiong, Shuangshuang Liu, Shipeng Zhang
Concrete and Cement Materials Research
article

CO₂ Seeding Admixtures for Enhanced Concrete Activation

Guangqi Xiong, Shuangshuang Liu, Shipeng Zhang
article en

Abstract

In this study, on-site CO2 seeding admixtures were prepared using power ultrasound-assisted pre-carbonation and chelator-assisted pre-carbonation (GLTA, EDTA) to enhance the carbonation efficiency and mechanical properties. Studies have shown that the application of power ultrasound can achieve a maximum CO2 uptake of 9.0% of the binder during the preacarbontion process. Compared with those of the traditional mixing batch and ordinary carbonation seeding activated batch, the strength of the power ultrasound seeding activated batch increased by 27.2 % and 21.4 %, respectively, after 1 day. Additionally, the EDTA-assisted pre-carbonation can achieve a maximum CO2 uptake of 9.6% of the binder during the preacarbontion process. Both early and later age strengths of cement mortar were enhanced by 21.33% at 1 day, 19.16% at 3 days, 16.00% at 7 days, and 16.38% at 28 days.

Hong Kong Polytechnic University
Openalex Percentile: Top 72%
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.