In situ synthesis of Fe–Mo alloys via synergistic smelting of copper slag and spent MoSi2 rods: Phase transformation and decomposition mechanism of MoSi2

The massive accumulation of copper slag and spent molybdenum disilicide rods results in significant waste of valuable metal elements such as Fe and Mo. To mitigate environmental pollution and promote metal recovery, this study proposes a synergistic smelting process for preparing ferromolybdenum alloy by utilizing spent molybdenum disilicide rods and copper slag. Through integrated analysis of thermodynamic simulations and non-isothermal kinetic experiments, the reduction behavior, phase reconstruction, and decomposition of MoSi 2 during the synergistic smelting process were systematically investigated. The magnetite phase and fayalite phase gradually decomposed under the influence of CaO and MoSi 2 , following the reaction pathways: Fe 3 O 4 →FeO→Fe and Fe 2 SiO 4 →Fe 1.5 Ca 0.5 (SiO 3 ) 2 →Fe. At approximately 950–1100 °C, an exothermic reaction occurred between MoSi 2 and copper slag, initiating in-situ formation of Fe 3 Mo. CaO improved the thermodynamic conditions and facilitated reaction progression. After system melting, solid-liquid reactions further decomposed MoSi 2 , while Mo and Si diffused into the slag, and Fe selectively captured Mo for directional enrichment. Differential scanning calorimetry analysis determined the activation energy for MoSi 2 -driven copper slag reduction to be 113.470 kJ/mol, confirming MoSi 2 as an efficient reductant. Under optimal temperature conditions, the recovery rates of Mo and Fe reached 99.21 % and 85.49 %, respectively, with Fe content in the secondary slag reduced to 4.04 %. This study utilizes spent molybdenum disilicide rods as both a reductant and a molybdenum source, without introducing carbon, providing a novel strategy for the high-value and low-carbon utilization of these two solid wastes.

Authors

Institutions

Publication Details

Journal
Journal of Materials Research and Technology
Published
2025-09-23
DOI
https://doi.org/10.1016/j.jmrt.2025.09.158
Citations
1
Primary Topic
Metallurgical and Alloy Processes
Type
article
Field-Weighted Citation Impact
2.93
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

In situ synthesis of Fe–Mo alloys via synergistic smelting of copper slag and spent MoSi2 rods: Phase transformation and decomposition mechanism of MoSi2

Baojing Zhang, Junxiu Li, Z.J. Zhang, Junsheng Cheng et al.
1 citations
Journal of Materials Research and Technology
Metallurgical and Alloy Processes
2.93
article

In situ synthesis of Fe–Mo alloys via synergistic smelting of copper slag and spent MoSi2 rods: Phase transformation and decomposition mechanism of MoSi2

Baojing Zhang, Junxiu Li, Z.J. Zhang, Junsheng Cheng, Shiheng Li, Peizhong Feng, Zhi Liu, Le Yu
article en
1 citations

Abstract

The massive accumulation of copper slag and spent molybdenum disilicide rods results in significant waste of valuable metal elements such as Fe and Mo. To mitigate environmental pollution and promote metal recovery, this study proposes a synergistic smelting process for preparing ferromolybdenum alloy by utilizing spent molybdenum disilicide rods and copper slag. Through integrated analysis of thermodynamic simulations and non-isothermal kinetic experiments, the reduction behavior, phase reconstruction, and decomposition of MoSi 2 during the synergistic smelting process were systematically investigated. The magnetite phase and fayalite phase gradually decomposed under the influence of CaO and MoSi 2 , following the reaction pathways: Fe 3 O 4 →FeO→Fe and Fe 2 SiO 4 →Fe 1.5 Ca 0.5 (SiO 3 ) 2 →Fe. At approximately 950–1100 °C, an exothermic reaction occurred between MoSi 2 and copper slag, initiating in-situ formation of Fe 3 Mo. CaO improved the thermodynamic conditions and facilitated reaction progression. After system melting, solid-liquid reactions further decomposed MoSi 2 , while Mo and Si diffused into the slag, and Fe selectively captured Mo for directional enrichment. Differential scanning calorimetry analysis determined the activation energy for MoSi 2 -driven copper slag reduction to be 113.470 kJ/mol, confirming MoSi 2 as an efficient reductant. Under optimal temperature conditions, the recovery rates of Mo and Fe reached 99.21 % and 85.49 %, respectively, with Fe content in the secondary slag reduced to 4.04 %. This study utilizes spent molybdenum disilicide rods as both a reductant and a molybdenum source, without introducing carbon, providing a novel strategy for the high-value and low-carbon utilization of these two solid wastes.

Journal of Materials Research and TechnologyVol. 39
China University of Mining and Technology (CN)
Openalex Percentile: Top 7%
Metallurgical and Alloy Processes
2.93
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.