Features of the Production Technology of Rolled Products from Boron Microalloyed Steels at a Casting and Rolling Complex
The paper presents the results of the development of technological modes for the production of hot-rolled coil products with a thickness of 9 mm from medium-carbon (0.20–0.34% C) low-alloy steels microalloyed with boron (0.002–0.005% B), and pipes made from them. The hot plasticity of steels at temperatures of 1200–700°C and deformation resistance at temperatures of 1100–700°C and deformation rates from 0.1 to 10 s–1 have been studied. Post-deformation cooling and heat treatment of the steels under study have been simulated under various conditions. The results of obtaining industrial samples of products with a temporary resistance of 1040–1050 MPa after heat treatment have been presented.
Authors
- A. S. Boiko
- А. V. Muntin (ORCID: https://orcid.org/0000-0002-8926-0110)
- S. D. Skachkov
- D. S. Astaf’ev
Institutions
- Moscow Power Engineering Institute (RU)
- Bauman Moscow State Technical University (RU)
- Moscow Aviation Institute (RU)
Publication Details
- Journal
- Steel in Translation
- Published
- 2025-05-01
- DOI
- https://doi.org/10.3103/s0967091225701049
- Primary Topic
- Metal Alloys Wear and Properties
- Type
- article
- Field-Weighted Citation Impact
- 0.00