Mechanical, Surface and Physicochemical Properties of Nanozeolite‐Modified <scp>3D</scp> Printed Hybrid Ceramics at Varying Concentrations: An In Vitro Study
Nanozeolite integration at 0.25% enhances strength, durability, and color stability in 3D-printed hybrid ceramics, improving their reliability for dental restorations. Higher loadings enhance surface properties but may modestly reduce bulk toughness and translucency, relevant for clinical decision-making.