Worse Interference of Fe <sup>3+</sup> than Fe <sup>2+</sup> on Degrading the Interphase and Performance of LiFePO <sub>4</sub> ||Graphite Battery

The detrimental effects of Fe-ion crosstalk on LiFePO<sub>4</sub>||Graphite battery performance, coupled with limited mechanistic insights into solid electrolyte interphase (SEI) evolution under such interference, warrant systematic investigation. Herein, advanced characterization techniques-including X-ray photoelectron spectroscopy, time-of-flight secondary ion mass spectrometry, and cryogenic transmission electron microscopy-are employed to reveal SEI evolution on graphite anodes under Fe<sup>2+</sup>/Fe<sup>3+</sup> influence. Results demonstrate that Fe<sup>3+</sup> exerts more severe adverse effects than Fe<sup>2+</sup>. Specifically, Fe<sup>2+</sup> primarily promotes conventional electrolyte reduction reactions, increasing H<sub>2</sub>, CH<sub>4</sub>, and CO<sub>2</sub> generation. In contrast, Fe<sup>3+</sup> facilitates radical combinations and catalyzes two-electron reductions, triggering side reactions releasing CO, C<sub>2</sub>H<sub>4</sub>, and C<sub>2</sub>H<sub>6</sub>. The SEI thickness under Fe-ion interference (Fe<sup>2+</sup>: 7.20-13.76 nm, Fe<sup>3+</sup>: 9.12-17.55 nm) significantly exceeds that of the base electrolyte (3.15-7.64 nm), with Fe deposits accumulating in organometallic forms. Critically, the presence of Fe<sup>3+</sup> and its adverse impacts on battery safety and cycling stability are validated in practical pouch cells. This study uncovers the chemical nature of the dissolved Fe ion and its deposits, provides mechanistic insights into its interference with SEI properties and Li-ion battery performances, which in turn helps to mitigate such detrimental effects.

Authors

Institutions

Publication Details

Journal
Advanced Materials
Published
2025-09-01
DOI
https://doi.org/10.1002/adma.202513736
Citations
8
Primary Topic
Advancements in Battery Materials
Type
article
Field-Weighted Citation Impact
5.84

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Worse Interference of Fe 3+ than Fe 2+ on Degrading the Interphase and Performance of LiFePO 4 ||Graphite Battery

Hao Zhang, Suting Weng, Yan Liu, Yejing Li et al.
8 citations
Advanced Materials
Advancements in Battery Materials
5.84
article

Worse Interference of Fe 3+ than Fe 2+ on Degrading the Interphase and Performance of LiFePO 4 ||Graphite Battery

Hao Zhang, Suting Weng, Yan Liu, Yejing Li, Cong Zhong, Qiu Fang, Xuefeng Wang, Jiacheng Zhu, Jiayi Zhang
article en
8 citations

Abstract

The detrimental effects of Fe-ion crosstalk on LiFePO<sub>4</sub>||Graphite battery performance, coupled with limited mechanistic insights into solid electrolyte interphase (SEI) evolution under such interference, warrant systematic investigation. Herein, advanced characterization techniques-including X-ray photoelectron spectroscopy, time-of-flight secondary ion mass spectrometry, and cryogenic transmission electron microscopy-are employed to reveal SEI evolution on graphite anodes under Fe<sup>2+</sup>/Fe<sup>3+</sup> influence. Results demonstrate that Fe<sup>3+</sup> exerts more severe adverse effects than Fe<sup>2+</sup>. Specifically, Fe<sup>2+</sup> primarily promotes conventional electrolyte reduction reactions, increasing H<sub>2</sub>, CH<sub>4</sub>, and CO<sub>2</sub> generation. In contrast, Fe<sup>3+</sup> facilitates radical combinations and catalyzes two-electron reductions, triggering side reactions releasing CO, C<sub>2</sub>H<sub>4</sub>, and C<sub>2</sub>H<sub>6</sub>. The SEI thickness under Fe-ion interference (Fe<sup>2+</sup>: 7.20-13.76 nm, Fe<sup>3+</sup>: 9.12-17.55 nm) significantly exceeds that of the base electrolyte (3.15-7.64 nm), with Fe deposits accumulating in organometallic forms. Critically, the presence of Fe<sup>3+</sup> and its adverse impacts on battery safety and cycling stability are validated in practical pouch cells. This study uncovers the chemical nature of the dissolved Fe ion and its deposits, provides mechanistic insights into its interference with SEI properties and Li-ion battery performances, which in turn helps to mitigate such detrimental effects.

Advanced MaterialsVol. 37(47)
Chinese Academy of Sciences (CN), Institute of Physics (CN), University of Chinese Academy of Sciences (CN), University of Science and Technology Beijing (CN)
National Natural Science Foundation of China, China Postdoctoral Science Foundation, National Key Research and Development Program of China
Openalex Percentile: Top 4%
Advancements in Battery Materials
5.84
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.