Behavior of Phosphorus During Selective Reduction of Iron from Oolitic Ore and Separation of Reduction Products

This study investigates the behavior of phosphorus during high-temperature smelting of hydrogen-reduced high-phosphorus oolitic iron ore from the Lisakovsk deposit. The preliminary reduction was carried out at temperatures ranging from 600 to 900 °C using hydrogen, aiming to selectively reduce iron to the metallic phase while retaining phosphorus in the oxide form. The resulting reduced products were subjected to wet magnetic separation and liquid-phase separation. It was found that neither method provides effective separation of phosphorus from iron: phosphorus partially enters the magnetic fraction and, during smelting, transfers into the metallic phase. To confirm the mechanism of phosphate reduction by metallic iron, a control experiment was conducted, in which a mixture of reduced iron and raw ore was smelted at 1650 °C. Microstructural and elemental analyses confirmed the redistribution of phosphorus into the metallic phase. These findings indicate that effective separation of iron and phosphorus cannot be achieved by reduction roasting alone and highlight the need for further studies on slag formation conditions and phase separation kinetics.

Authors

Institutions

Publication Details

Journal
Materials
Published
2025-08-29
DOI
https://doi.org/10.3390/ma18174051
Primary Topic
Iron and Steelmaking Processes
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Behavior of Phosphorus During Selective Reduction of Iron from Oolitic Ore and Separation of Reduction Products

Yerbol Kuatbay, K. I. Smirnov, П. А. Гамов, N. Kosdauletov et al.
Materials
Iron and Steelmaking Processes
article

Behavior of Phosphorus During Selective Reduction of Iron from Oolitic Ore and Separation of Reduction Products

Yerbol Kuatbay, K. I. Smirnov, П. А. Гамов, N. Kosdauletov, Б. Сулеймен, Almas Yerzhanov, Bauyrzhan Kelamanov, Galymzhan Adilov, Assylbek Abdirashit, Assylbek Nurumgaliyev, Talgat Zhuniskaliyev, Assemay Pushanova
article en

Abstract

This study investigates the behavior of phosphorus during high-temperature smelting of hydrogen-reduced high-phosphorus oolitic iron ore from the Lisakovsk deposit. The preliminary reduction was carried out at temperatures ranging from 600 to 900 °C using hydrogen, aiming to selectively reduce iron to the metallic phase while retaining phosphorus in the oxide form. The resulting reduced products were subjected to wet magnetic separation and liquid-phase separation. It was found that neither method provides effective separation of phosphorus from iron: phosphorus partially enters the magnetic fraction and, during smelting, transfers into the metallic phase. To confirm the mechanism of phosphate reduction by metallic iron, a control experiment was conducted, in which a mixture of reduced iron and raw ore was smelted at 1650 °C. Microstructural and elemental analyses confirmed the redistribution of phosphorus into the metallic phase. These findings indicate that effective separation of iron and phosphorus cannot be achieved by reduction roasting alone and highlight the need for further studies on slag formation conditions and phase separation kinetics.

MaterialsVol. 18(17)
South Ural State University (RU), Aktobe Regional State University named after K.Zhubanov (KZ), Karaganda State Industrial University (KZ)
Openalex Percentile: Top 77%
Iron and Steelmaking Processes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.