Electrochemical machining of groove on tungsten using bipolar pulses and auxiliary electrode

Electrochemical machining (ECM) directly controls the dissolution of anodic materials in the fabrication of metallic parts. The electrochemical dissolution behavior of the workpiece material is determined by its electrochemical properties rather than its hardness. Consequently, it is easy to machine difficult-to-cut materials such as tungsten. However, conventional ECM using a unipolar pulse (UP-ECM) and a neutral electrolyte (NaNO 3 aq) is difficult to machine tungsten, because tungsten oxide (WO 3 ) with a high impedance is generated in the machining area, which hinders the further dissolution of tungsten. In our previous study, an ECM method using bipolar pulses and an auxiliary electrode (BPAE-ECM) was used to induce intensive hydrogen bubbles, thereby reducing stray corrosion. In this study, this method was used to remove WO 3 and machine grooves on tungsten. During the negative pulse period, the workpiece acts as the cathode and generates hydroxide ions (OH - ) from hydrogen evolution to dissolve WO 3 , allowing the process to continue. Based on this theory, ECM experiments were conducted to investigate the machining characteristics of tungsten.

Authors

Institutions

Publication Details

Journal
Procedia CIRP
Published
2025-01-01
DOI
https://doi.org/10.1016/j.procir.2025.06.008
Primary Topic
Advanced Machining and Optimization Techniques
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Electrochemical machining of groove on tungsten using bipolar pulses and auxiliary electrode

Wataru Natsu, Zehao Huang, Hongping Luo, Qingrong Zhang
Procedia CIRP
Advanced Machining and Optimization Techniques
article

Electrochemical machining of groove on tungsten using bipolar pulses and auxiliary electrode

Wataru Natsu, Zehao Huang, Hongping Luo, Qingrong Zhang
article en

Abstract

Electrochemical machining (ECM) directly controls the dissolution of anodic materials in the fabrication of metallic parts. The electrochemical dissolution behavior of the workpiece material is determined by its electrochemical properties rather than its hardness. Consequently, it is easy to machine difficult-to-cut materials such as tungsten. However, conventional ECM using a unipolar pulse (UP-ECM) and a neutral electrolyte (NaNO 3 aq) is difficult to machine tungsten, because tungsten oxide (WO 3 ) with a high impedance is generated in the machining area, which hinders the further dissolution of tungsten. In our previous study, an ECM method using bipolar pulses and an auxiliary electrode (BPAE-ECM) was used to induce intensive hydrogen bubbles, thereby reducing stray corrosion. In this study, this method was used to remove WO 3 and machine grooves on tungsten. During the negative pulse period, the workpiece acts as the cathode and generates hydroxide ions (OH - ) from hydrogen evolution to dissolve WO 3 , allowing the process to continue. Based on this theory, ECM experiments were conducted to investigate the machining characteristics of tungsten.

Procedia CIRPVol. 137
Guangdong University of Technology (CN), Tokyo University of Agriculture and Technology (JP)
Machine Tool Engineering Foundation
Openalex Percentile: Top 78%
Advanced Machining and Optimization Techniques
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Electrochemical machining of groove on tungsten using bipolar pulses and auxiliary electrode — Wataru Natsu, Zehao Huang, et al. · Procedia CIRP (2025) | TGRS Research Map | TGRS