Non-flammable polymeric ionic liquid hybrid electrolytes for high-stability solid-state sodium metal batteries

Solid-state sodium metal batteries (SMBs) show promise for next-generation energy storage, but challenges remain in developing electrolytes that balance safety, performance, and longevity. This study introduces a hybrid electrolyte system for SMBs, combining a poly(diallyldimethylammonium) bis(fluorosulfonyl)imide polymer matrix with a sodium bis(fluorosulfonyl)imide in N-butyl- N -methylpyrrolidinium bis(trifluoromethyl sulfonyl)imide ionic liquid electrolyte. The optimized hybrid electrolyte exhibits a sodium ion conductivity of 2.1 mS cm −1 at 70 °C and an oxidative stability of 4.8 V vs Na + /Na. Electrochemical characterization reveals efficient sodium plating/stripping with a critical current density of 8.5 mA cm −2 . X-ray photoelectron spectroscopy identifies a NaF-rich interphase at the sodium metal surface, contributing to interfacial stability. An all-solid-state SMB utilizing this electrolyte and a sodium vanadium phosphate cathode demonstrates stable cycling at 60 °C, retaining 75 % capacity after 2000 cycles. These results highlight the potential of hybrid electrolytes in advancing safe, high-performance solid-state SMBs for future energy storage applications. • Non-flammable PDADMAFSI-ionic liquid hybrid electrolyte for sodium metal batteries • Achieves 2.1 mS cm −1 Na + conductivity at 70 °C and 4.8 V vs Na + /Na oxidative stability • Enables stable Na plating/stripping with 8.5 mA/cm 2 critical current density • XPS reveals NaF-rich interphase that enhances interfacial and cycling stability. • Full cells retain 75 % capacity after 2000 cycles at 60 °C with NVP cathode.

Authors

Institutions

Publication Details

Journal
Chemical Engineering Journal
Published
2025-08-25
DOI
https://doi.org/10.1016/j.cej.2025.167657
Citations
2
Primary Topic
Advanced Battery Materials and Technologies
Type
article
Field-Weighted Citation Impact
1.46

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Non-flammable polymeric ionic liquid hybrid electrolytes for high-stability solid-state sodium metal batteries

Eldho Edison, Victor Mougel, Daniel F. Abbott, Shivaprakash N. Ramakrishna et al.
2 citations
Chemical Engineering Journal
Advanced Battery Materials and Technologies
1.46
article

Non-flammable polymeric ionic liquid hybrid electrolytes for high-stability solid-state sodium metal batteries

Eldho Edison, Victor Mougel, Daniel F. Abbott, Shivaprakash N. Ramakrishna, Markus Niederberger
article en
2 citations

Abstract

Solid-state sodium metal batteries (SMBs) show promise for next-generation energy storage, but challenges remain in developing electrolytes that balance safety, performance, and longevity. This study introduces a hybrid electrolyte system for SMBs, combining a poly(diallyldimethylammonium) bis(fluorosulfonyl)imide polymer matrix with a sodium bis(fluorosulfonyl)imide in N-butyl- N -methylpyrrolidinium bis(trifluoromethyl sulfonyl)imide ionic liquid electrolyte. The optimized hybrid electrolyte exhibits a sodium ion conductivity of 2.1 mS cm −1 at 70 °C and an oxidative stability of 4.8 V vs Na + /Na. Electrochemical characterization reveals efficient sodium plating/stripping with a critical current density of 8.5 mA cm −2 . X-ray photoelectron spectroscopy identifies a NaF-rich interphase at the sodium metal surface, contributing to interfacial stability. An all-solid-state SMB utilizing this electrolyte and a sodium vanadium phosphate cathode demonstrates stable cycling at 60 °C, retaining 75 % capacity after 2000 cycles. These results highlight the potential of hybrid electrolytes in advancing safe, high-performance solid-state SMBs for future energy storage applications. • Non-flammable PDADMAFSI-ionic liquid hybrid electrolyte for sodium metal batteries • Achieves 2.1 mS cm −1 Na + conductivity at 70 °C and 4.8 V vs Na + /Na oxidative stability • Enables stable Na plating/stripping with 8.5 mA/cm 2 critical current density • XPS reveals NaF-rich interphase that enhances interfacial and cycling stability. • Full cells retain 75 % capacity after 2000 cycles at 60 °C with NVP cathode.

Chemical Engineering JournalVol. 522
ETH Zurich (CH)
Eidgenössische Technische Hochschule Zürich
Affordable and clean energy
Openalex Percentile: Top 15%
Advanced Battery Materials and Technologies
1.46
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.