Preparation of Ni-P Composite Coatings and Study on the Corrosion Resistance and Antifouling Properties in Low-Temperature Flue Gas Environment

In industrial production, flue gas heat exchangers are often affected by the low-temperature condensation of industrial flue gas due to the influence of the working environment, resulting in serious ash deposition and corrosion. In order to solve this problem, in this study, we developed an ash deposition and corrosion monitoring system to compare the ash deposition prevention performance and corrosion resistance of different materials, as well as its influence on the heat transfer performance of different materials in the same environment. The following coatings were selected for the experiment (values in parentheses are the concentrations of the added compounds): ND, Q235, 316L, Ni-Cu (0.4 g/L)-P, Ni-P-SiO<sub>2</sub> (40 g/L), Ni-Cu (0.4 g/L)-P-SiO<sub>2</sub> (20 g/L), Ni-Cu (0.4 g/L)-P-SiO<sub>2</sub> (40 g/L), and Ni-Cu (0.4 g/L)-P-SiO<sub>2</sub> (60 g/L). The results show that the Ni-Cu (0.4 g/L)-P-SiO<sub>2</sub> (40 g/L) coating has excellent corrosion resistance, while the Ni-Cu (0.4 g/L)-P-SiO<sub>2</sub> (60 g/L) coating shows excellent antifouling performance. Through the comparative analysis of polarization curves, impedance spectra, and coupled corrosion experiments, the test materials were ranked as follows based on their corrosion resistance: 316L > Ni-Cu-P-SiO<sub>2</sub> (40 g/L) > Ni-Cu-P-SiO<sub>2</sub> (20 g/L) > Ni-P-SiO<sub>2</sub> > Ni-Cu-P-SiO<sub>2</sub> (60 g/L) > Ni-Cu-P > ND > Q235. It was also demonstrated that the new coated pipes were able to reduce the exhaust temperature below the dew point and maximize the recovery of energy from the exhaust gas. The acid-ash coupling mechanism of the coating in the flue gas environment was further analyzed, and an acid-ash coupling model based on Cu and SiO<sub>2</sub> is proposed. This model analyzes the effect of the coating under the acid-ash coupling mechanism. Using coated tubes in heat exchangers helps to recover waste heat from coal-fired boilers, enhance heat exchange efficiency, extend the service life of heat exchangers, and reduce costs.

Authors

Institutions

Publication Details

Journal
Materials
Published
2025-08-22
DOI
https://doi.org/10.3390/ma18173939
Primary Topic
High-Temperature Coating Behaviors
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Preparation of Ni-P Composite Coatings and Study on the Corrosion Resistance and Antifouling Properties in Low-Temperature Flue Gas Environment

Shengxian Cao, Bo Zhao, Changqi Lv, Xi Yu
Materials
High-Temperature Coating Behaviors
article

Preparation of Ni-P Composite Coatings and Study on the Corrosion Resistance and Antifouling Properties in Low-Temperature Flue Gas Environment

Shengxian Cao, Bo Zhao, Changqi Lv, Xi Yu
article en

Abstract

In industrial production, flue gas heat exchangers are often affected by the low-temperature condensation of industrial flue gas due to the influence of the working environment, resulting in serious ash deposition and corrosion. In order to solve this problem, in this study, we developed an ash deposition and corrosion monitoring system to compare the ash deposition prevention performance and corrosion resistance of different materials, as well as its influence on the heat transfer performance of different materials in the same environment. The following coatings were selected for the experiment (values in parentheses are the concentrations of the added compounds): ND, Q235, 316L, Ni-Cu (0.4 g/L)-P, Ni-P-SiO<sub>2</sub> (40 g/L), Ni-Cu (0.4 g/L)-P-SiO<sub>2</sub> (20 g/L), Ni-Cu (0.4 g/L)-P-SiO<sub>2</sub> (40 g/L), and Ni-Cu (0.4 g/L)-P-SiO<sub>2</sub> (60 g/L). The results show that the Ni-Cu (0.4 g/L)-P-SiO<sub>2</sub> (40 g/L) coating has excellent corrosion resistance, while the Ni-Cu (0.4 g/L)-P-SiO<sub>2</sub> (60 g/L) coating shows excellent antifouling performance. Through the comparative analysis of polarization curves, impedance spectra, and coupled corrosion experiments, the test materials were ranked as follows based on their corrosion resistance: 316L > Ni-Cu-P-SiO<sub>2</sub> (40 g/L) > Ni-Cu-P-SiO<sub>2</sub> (20 g/L) > Ni-P-SiO<sub>2</sub> > Ni-Cu-P-SiO<sub>2</sub> (60 g/L) > Ni-Cu-P > ND > Q235. It was also demonstrated that the new coated pipes were able to reduce the exhaust temperature below the dew point and maximize the recovery of energy from the exhaust gas. The acid-ash coupling mechanism of the coating in the flue gas environment was further analyzed, and an acid-ash coupling model based on Cu and SiO<sub>2</sub> is proposed. This model analyzes the effect of the coating under the acid-ash coupling mechanism. Using coated tubes in heat exchangers helps to recover waste heat from coal-fired boilers, enhance heat exchange efficiency, extend the service life of heat exchangers, and reduce costs.

MaterialsVol. 18(17)
Northeast Electric Power University (CN)
Jilin Scientific and Technological Development Program
Openalex Percentile: Top 70%
High-Temperature Coating Behaviors
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.