Effect of Coarse Aggregate Dimensional Variation On The Compressive Strength of Concrete

In the world of construction, concrete has a very important function as the main material due to its role in maintaining the strength and stability of the structure. This study aims to evaluate the effect of coarse aggregate size variations on the compressive strength of concrete and determine the most suitable size for use. The use of coarse aggregates is focused on granules that are retained on 3/4-inch and 3/8-inch sieves. The results showed that concrete with coarse aggregate retained in a 3/8 inch sieve had a higher compressive strength than 3/4 inch aggregate. At 3 days of age, the average compressive strength value reached 12,078 MPa for 3/8 inch coarse aggregate and 10,587 MPa for 3/4 inch aggregate. This difference continued at the 28-day lifetime compressive strength (the result of the 1971 PBI conversion), which was with an average value of 30,296 MPa for a 3/8 inch aggregate and 26,469 MPa for a 3/4 inch aggregate. This difference is due to a tighter distribution of patricles, reduced pore volume, and more optimal bonding of cement paste and aggregate. Therefore, the selection of coarse aggregate sizes needs to be adjusted to the purpose of construction.

Authors

Institutions

Publication Details

Journal
International Journal of Science and Environment (IJSE)
Published
2025-08-16
DOI
https://doi.org/10.51601/ijse.v5i3.212
Primary Topic
Innovative concrete reinforcement materials
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Effect of Coarse Aggregate Dimensional Variation On The Compressive Strength of Concrete

Adryan Fitrayudha, Hafiz Hamdani, Yogika Oktavian
5 links
International Journal of Science and Environment (IJSE)
Innovative concrete reinforcement materials
article

Effect of Coarse Aggregate Dimensional Variation On The Compressive Strength of Concrete

Adryan Fitrayudha, Hafiz Hamdani, Yogika Oktavian
article en

Abstract

In the world of construction, concrete has a very important function as the main material due to its role in maintaining the strength and stability of the structure. This study aims to evaluate the effect of coarse aggregate size variations on the compressive strength of concrete and determine the most suitable size for use. The use of coarse aggregates is focused on granules that are retained on 3/4-inch and 3/8-inch sieves. The results showed that concrete with coarse aggregate retained in a 3/8 inch sieve had a higher compressive strength than 3/4 inch aggregate. At 3 days of age, the average compressive strength value reached 12,078 MPa for 3/8 inch coarse aggregate and 10,587 MPa for 3/4 inch aggregate. This difference continued at the 28-day lifetime compressive strength (the result of the 1971 PBI conversion), which was with an average value of 30,296 MPa for a 3/8 inch aggregate and 26,469 MPa for a 3/4 inch aggregate. This difference is due to a tighter distribution of patricles, reduced pore volume, and more optimal bonding of cement paste and aggregate. Therefore, the selection of coarse aggregate sizes needs to be adjusted to the purpose of construction.

International Journal of Science and Environment (IJSE)Vol. 5(3)
University of Muhammadiyah Mataram (ID)
Openalex Percentile: Top 78%
Innovative concrete reinforcement materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.