Freeze–thaw–induced microstructural alterations and deterioration of physicomechanical properties in rocks from the Himalayan ranges (Pakistan)

This study investigates in detail the impact of freeze-thaw cycles on the physical and mechanical properties of a variety of rock types, including granulite, amphibolite, limestone, sandstone, granitic gneiss, quartzite, rhyolite, dolerite, and gabbronorite. The selected rock samples underwent several freeze-thaw cycles at temperatures ranging from 25°C to -40°C. After these cycles, tests were performed to assess the response of the rocks to varying temperatures. Destructive tests (uniaxial compressive strength, point load index) and non-destructive testing (specific gravity, ultrasonic pulse wave velocity, porosity, and water absorption) were carried out. The density of the induced fractures in each type of rock under investigation was calculated. The fracture density in the samples increased as the number of cycles increased. After fifty cycles, the fracture density of selected rocks increased as follows: 1.12% for sandstone, 1.06% for limestone, 0.59% for rhyolite, 0.48% for gabbronorite, 0.57% for quartzite, 0.76% for granitic gneiss, 0.46% for amphibolite, and 0.43% for granulite. The extent and strength of the fractures increased further with continued cycles. After 100 freeze-thaw cycles, the fracture densities rose to 1.47%, 1.44%, 1.22%, 1.05%, 1.14%, 1.31%, 1.03%, and 1.02%, respectively. Similarly, porosity and water absorption levels showed an increased trend. However, as the freeze-thaw process continues, the results indicate a decrease in uniaxial compressive strength (UCS), specific gravity, ultrasonic pulse velocity (UPV), and point load strength. These findings highlight how freeze-thaw conditions deteriorate rocks and change their physico-mechanical characteristics, with significant implications for the mining and building sectors.

Authors

Institutions

Publication Details

Journal
Earth Sciences Research Journal
Published
2025-04-21
DOI
https://doi.org/10.15446/esrj.v29n1.116550
Citations
2
Primary Topic
Climate change and permafrost
Type
article
Field-Weighted Citation Impact
2.60

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Freeze–thaw–induced microstructural alterations and deterioration of physicomechanical properties in rocks from the Himalayan ranges (Pakistan)

Muhammad Sajid, Abdul Rahim Asif, Abid Nawaz, Waqas Ahmed
2 citations
Earth Sciences Research Journal
Climate change and permafrost
2.60
article

Freeze–thaw–induced microstructural alterations and deterioration of physicomechanical properties in rocks from the Himalayan ranges (Pakistan)

Muhammad Sajid, Abdul Rahim Asif, Abid Nawaz, Waqas Ahmed
article en
2 citations

Abstract

This study investigates in detail the impact of freeze-thaw cycles on the physical and mechanical properties of a variety of rock types, including granulite, amphibolite, limestone, sandstone, granitic gneiss, quartzite, rhyolite, dolerite, and gabbronorite. The selected rock samples underwent several freeze-thaw cycles at temperatures ranging from 25°C to -40°C. After these cycles, tests were performed to assess the response of the rocks to varying temperatures. Destructive tests (uniaxial compressive strength, point load index) and non-destructive testing (specific gravity, ultrasonic pulse wave velocity, porosity, and water absorption) were carried out. The density of the induced fractures in each type of rock under investigation was calculated. The fracture density in the samples increased as the number of cycles increased. After fifty cycles, the fracture density of selected rocks increased as follows: 1.12% for sandstone, 1.06% for limestone, 0.59% for rhyolite, 0.48% for gabbronorite, 0.57% for quartzite, 0.76% for granitic gneiss, 0.46% for amphibolite, and 0.43% for granulite. The extent and strength of the fractures increased further with continued cycles. After 100 freeze-thaw cycles, the fracture densities rose to 1.47%, 1.44%, 1.22%, 1.05%, 1.14%, 1.31%, 1.03%, and 1.02%, respectively. Similarly, porosity and water absorption levels showed an increased trend. However, as the freeze-thaw process continues, the results indicate a decrease in uniaxial compressive strength (UCS), specific gravity, ultrasonic pulse velocity (UPV), and point load strength. These findings highlight how freeze-thaw conditions deteriorate rocks and change their physico-mechanical characteristics, with significant implications for the mining and building sectors.

Earth Sciences Research JournalVol. 29(1)
University of Peshawar (PK)
University of Peshawar
Openalex Percentile: Top 10%
Climate change and permafrost
2.60
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.