First result of boronization assisted by the ICWC on EAST with full metal wall

Abstract Boron (B), a low-Z (atomic number) material, has been widely utilized in wall conditioning to improve plasma performance in fusion devices [1]. In 2023, boronization was successfully conducted on EAST featuring an ITER-like tungsten divertor and fully metallic first wall. The process employed predischarge coating with carborane (C2B10H12) as the working material, assisted by ion cyclotron wall conditioning (ICWC). After one time 12 g boronization, it was found the thickness of B film was approximately 120 nm. Post-boronization observations indicated that substantial hydrogen (H) release during initial plasma discharges compared with the consumed W/B wall, attributed to H co-deposition during the ICWC-boronization processing, which led to uncontrollable divertor neutral pressure and plasma density. The H/(H+D) ratio demonstrated a gradual reduction from ~85% to 30% over more than 1850 s of deuterium plasma, with a cumulative injected energy of 2325 MJ. The B coating significantly enhanced the stored energy in plasma and improved confinement performance. The stored energy in plasma showed an increase of about 20%, primarily due to a reduction in impurity radiation, including oxygen (O) and heavy impurities such as tungsten (W), iron (Fe), and copper (Cu). The effective ion charge (Zeff) decreased from 2.3 to 2.0. Following ICWC-boronization, the line-integrated radiation profile decreased by nearly 35% in the plasma core, plasma density and electron temperature exhibited an increase of ~7% and 12% due to enhanced wall fueling and reduced impurity radiation. The lifetime of boronization, as evaluated by the line emissions from boron and other impurity radiation, was about 1700 seconds of deuterium plasma, with a cumulative injected energy of 2125 MJ on EAST. These findings provide significant insights for evaluating ICWC-boronization applicability in ITER with full W wall structure.

Authors

Institutions

Publication Details

Journal
Nuclear Fusion
Published
2025-08-04
DOI
https://doi.org/10.1088/1741-4326/adf75c
Citations
1
Primary Topic
Fusion materials and technologies
Type
article
Field-Weighted Citation Impact
0.52

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

First result of boronization assisted by the ICWC on EAST with full metal wall

T. Wauters, Yue Guan, Tianqi Jia, Zhe Wang et al.
1 citations
Nuclear Fusion
Fusion materials and technologies
0.52
article

First result of boronization assisted by the ICWC on EAST with full metal wall

T. Wauters, Yue Guan, Tianqi Jia, Zhe Wang, Guizhong Zuo, Lili Wang, Tao Zhang, Ling Zhang, Rui Ding, Wei Xu, Zhen Sun, Jiang Hu, Hailin Zhao, Songtao Mao, Xianzu Gong, Yaowei Yu, Zhenwei Wu, Shouan Puyang
article en
1 citations

Abstract

Abstract Boron (B), a low-Z (atomic number) material, has been widely utilized in wall conditioning to improve plasma performance in fusion devices [1]. In 2023, boronization was successfully conducted on EAST featuring an ITER-like tungsten divertor and fully metallic first wall. The process employed predischarge coating with carborane (C2B10H12) as the working material, assisted by ion cyclotron wall conditioning (ICWC). After one time 12 g boronization, it was found the thickness of B film was approximately 120 nm. Post-boronization observations indicated that substantial hydrogen (H) release during initial plasma discharges compared with the consumed W/B wall, attributed to H co-deposition during the ICWC-boronization processing, which led to uncontrollable divertor neutral pressure and plasma density. The H/(H+D) ratio demonstrated a gradual reduction from ~85% to 30% over more than 1850 s of deuterium plasma, with a cumulative injected energy of 2325 MJ. The B coating significantly enhanced the stored energy in plasma and improved confinement performance. The stored energy in plasma showed an increase of about 20%, primarily due to a reduction in impurity radiation, including oxygen (O) and heavy impurities such as tungsten (W), iron (Fe), and copper (Cu). The effective ion charge (Zeff) decreased from 2.3 to 2.0. Following ICWC-boronization, the line-integrated radiation profile decreased by nearly 35% in the plasma core, plasma density and electron temperature exhibited an increase of ~7% and 12% due to enhanced wall fueling and reduced impurity radiation. The lifetime of boronization, as evaluated by the line emissions from boron and other impurity radiation, was about 1700 seconds of deuterium plasma, with a cumulative injected energy of 2125 MJ on EAST. These findings provide significant insights for evaluating ICWC-boronization applicability in ITER with full W wall structure.

Nuclear Fusion
ITER (FR), University of Science and Technology of China (CN), Chinese Academy of Sciences (CN), Princeton University (US), Princeton Plasma Physics Laboratory (US), Hefei Institutes of Physical Science (CN), Institute of Plasma Physics (CN)
National Natural Science Foundation of China, National Key Research and Development Program of China
Openalex Percentile: Top 35%
Fusion materials and technologies
0.52
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.