Electron Transport Characteristics of Photosensitive Al/ZnO/Pt Schottky Junction Fabricated on (002) Oriented Pulsed Laser‐Deposited ZnO Thin Film

Herein, pulsed laser‐deposited ZnO thin‐film‐based devices have been extensively studied in terms of their structural, dielectric, and electron transport properties. Structural analysis using X‐ray diffraction reveals that the deposited film has a preferred (002) orientation with an average crystallite size of 20.05 nm, calculated by Debye–Scherrer formula. Using the deposited ZnO layer, Al/ZnO/Pt‐based metal–semiconductor–metal junction has been prepared. From room temperature DC current–voltage characteristics, the illuminated Al/ZnO junction's calculated Schottky barrier height is found to be 0.78 eV with a high ideality factor of 6.92. The fabricated device is found to be photosensitive in nature, with measured response and recovery time of 0.93 s and 0.55 s, respectively, when illuminated by a light‐emitting diode overhead flashlight.

Authors

Institutions

Publication Details

Journal
physica status solidi (a)
Published
2025-08-04
DOI
https://doi.org/10.1002/pssa.202500280
Primary Topic
ZnO doping and properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Electron Transport Characteristics of Photosensitive Al/ZnO/Pt Schottky Junction Fabricated on (002) Oriented Pulsed Laser‐Deposited ZnO Thin Film

A. Venimadhav, Gourab Bhattacharya, Ronit Hindoddikar
physica status solidi (a)
ZnO doping and properties
article

Electron Transport Characteristics of Photosensitive Al/ZnO/Pt Schottky Junction Fabricated on (002) Oriented Pulsed Laser‐Deposited ZnO Thin Film

A. Venimadhav, Gourab Bhattacharya, Ronit Hindoddikar
article en

Abstract

Herein, pulsed laser‐deposited ZnO thin‐film‐based devices have been extensively studied in terms of their structural, dielectric, and electron transport properties. Structural analysis using X‐ray diffraction reveals that the deposited film has a preferred (002) orientation with an average crystallite size of 20.05 nm, calculated by Debye–Scherrer formula. Using the deposited ZnO layer, Al/ZnO/Pt‐based metal–semiconductor–metal junction has been prepared. From room temperature DC current–voltage characteristics, the illuminated Al/ZnO junction's calculated Schottky barrier height is found to be 0.78 eV with a high ideality factor of 6.92. The fabricated device is found to be photosensitive in nature, with measured response and recovery time of 0.93 s and 0.55 s, respectively, when illuminated by a light‐emitting diode overhead flashlight.

physica status solidi (a)Vol. 222(17)
Indian Institute of Technology Kharagpur (IN)
Openalex Percentile: Top 86%
ZnO doping and properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Electron Transport Characteristics of Photosensitive Al/ZnO/Pt Schottky Junction Fabricated on (002) Oriented Pulsed Laser‐Deposited ZnO Thin Film — A. Venimadhav, Gourab Bhattacharya, et al. · physica status solidi (a) (2025) | TGRS Research Map | TGRS