Effect of thermocycling and surface treatments on the bond strength of a hybrid PICN ceramic.
Cementation of a hybrid ceramic treated with sandblasting, silane and a 10-MDP-based adhesive ensures high bond values, even when aged under hot, humid conditions. Thermocycling significantly reduced the adhesive strength in all groups, the decrease being more noticeable in those that did not include silane.
Authors
- Inés Villacís-Altamirano (ORCID: https://orcid.org/0000-0002-3994-2121)
- Marcelo Geovanny Cascante Calderón (ORCID: https://orcid.org/0000-0003-3474-6196)
- Alexandra Salinas (ORCID: https://orcid.org/0000-0001-9042-9190)
- A. Flores (ORCID: https://orcid.org/0000-0003-4926-0869)
Institutions
- Central University of Ecuador (EC)
Publication Details
- Journal
- PubMed
- Published
- 2025-04-01
- DOI
- https://doi.org/10.54589/aol.38/1/69
- Primary Topic
- Dental materials and restorations
- Type
- article
- Field-Weighted Citation Impact
- 0.00