Pengaruh Penggunaan Batu Kapur dari Wilayah Sampung Kabupaten Ponorogo Sebagai Pengganti Agregat Kasar Terhadap Kuat Tekan Beton

Ponorogo, renowned for its abundant mineral resources such as limestone, presents an opportunity to utilize this material as a substitute for coarse aggregate in concrete mixtures. This research investigated the impact of replacing coarse aggregate with Sampung limestone at concentrations of 0%, 25%, 50%, 75%, and 100%. Following the Department of Environment (DoE) method and referencing SNI 03-2834-2000 for concrete mix design, 28-day compressive strength tests yielded results of 14.35 MPa for 0% limestone, 12.96 MPa for 25%, 14.35 MPa for 50%, 12.03 MPa for 75%, and 10.65 MPa for 100%. Remarkably, the findings indicate that the 50% limestone mixture achieved the most optimal compressive strength.

Authors

Institutions

Publication Details

Journal
Jurnal Teknik Industri Terintegrasi
Published
2025-07-04
DOI
https://doi.org/10.31004/jutin.v8i3.45636
Primary Topic
Geotechnical and construction materials studies
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Pengaruh Penggunaan Batu Kapur dari Wilayah Sampung Kabupaten Ponorogo Sebagai Pengganti Agregat Kasar Terhadap Kuat Tekan Beton

Aulia Bintang Mahanani, Nurul Rochmah
Jurnal Teknik Industri Terintegrasi
Geotechnical and construction materials studies
article

Pengaruh Penggunaan Batu Kapur dari Wilayah Sampung Kabupaten Ponorogo Sebagai Pengganti Agregat Kasar Terhadap Kuat Tekan Beton

Aulia Bintang Mahanani, Nurul Rochmah
article en

Abstract

Ponorogo, renowned for its abundant mineral resources such as limestone, presents an opportunity to utilize this material as a substitute for coarse aggregate in concrete mixtures. This research investigated the impact of replacing coarse aggregate with Sampung limestone at concentrations of 0%, 25%, 50%, 75%, and 100%. Following the Department of Environment (DoE) method and referencing SNI 03-2834-2000 for concrete mix design, 28-day compressive strength tests yielded results of 14.35 MPa for 0% limestone, 12.96 MPa for 25%, 14.35 MPa for 50%, 12.03 MPa for 75%, and 10.65 MPa for 100%. Remarkably, the findings indicate that the 50% limestone mixture achieved the most optimal compressive strength.

Jurnal Teknik Industri TerintegrasiVol. 8(3)
Universitas 17 Agustus 1945 Surabaya (ID)
Openalex Percentile: Top 82%
Geotechnical and construction materials studies
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.