Structural and Dynamic Origins of Payne Effect Reduction by Steric Stabilization in Silica Reinforced Poly(butadiene) Nanocomposites

ABSTRACT Silica nanoparticles in polybutadiene nanocomposites cause significantly hindered polymer dynamics in the form of a glassy layer, which can extend more than 10 nm from the nanoparticle surface. We present experiments for a well‐defined series of these nanocomposites to contrast the contributions of free chain ends versus hindered dynamics on the non‐linear rheological effects associated with energy loss in transport. Quasi‐elastic neutron scattering (QENS) experiments using isotopic labeling and interfacially‐active polymers enabled quantification of the glassy layer's thickness, which we relate to the strain softening (Payne effect), energy dissipation and the previously established nanostructure of the materials. We explored the thickness of the glassy layer from near the bulk glass transition temperature up to 363 K, in the presence or absence of nanoparticles and interfacially active polymers. Although the glassy layer becomes thinner with increasing temperature, it remains significant (> 3 nm) even when the sample is more than 180 K above the bulk glass transition temperature. This layer can account for the substantial levels of reinforcement, up to a factor of 20, and energy dissipation observed in silica filled rubbers beyond values expected from particle volume fraction arguments alone. Since the interfacially‐active polymers simultaneously inhibit nanoparticle aggregation and introduce polymer chain ends to the interparticle region, these experiments provide a direct test of whether energy loss in reinforced nanocomposites is attributable to “glassy bridges” between particles or chain ends. We show that while chain ends may be significant at low strain, below 1%, the percolation of the glassy layer of hindered polymer dynamics between silica particles dominates the Payne effect at high strain (~10% or more) and that this contribution can be dramatically reduced by sufficient steric stabilization to the nanoparticles.

Authors

Institutions

Publication Details

Journal
Polymer Composites
Published
2025-07-12
DOI
https://doi.org/10.1002/pc.70163
Citations
1
Primary Topic
Polymer Nanocomposites and Properties
Type
article
Field-Weighted Citation Impact
0.61

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Structural and Dynamic Origins of Payne Effect Reduction by Steric Stabilization in Silica Reinforced Poly(butadiene) Nanocomposites

Nigel Clarke, Lian R. Hutchings, Victoria García Sakai, B. Frick et al.
1 citations
Polymer Composites
Polymer Nanocomposites and Properties
0.61
article

Structural and Dynamic Origins of Payne Effect Reduction by Steric Stabilization in Silica Reinforced Poly(butadiene) Nanocomposites

Nigel Clarke, Lian R. Hutchings, Victoria García Sakai, B. Frick, W. Douglas Carswell, Richard L. Thompson, Stephen C. Boothroyd, James M. Hart
article en
1 citations

Abstract

ABSTRACT Silica nanoparticles in polybutadiene nanocomposites cause significantly hindered polymer dynamics in the form of a glassy layer, which can extend more than 10 nm from the nanoparticle surface. We present experiments for a well‐defined series of these nanocomposites to contrast the contributions of free chain ends versus hindered dynamics on the non‐linear rheological effects associated with energy loss in transport. Quasi‐elastic neutron scattering (QENS) experiments using isotopic labeling and interfacially‐active polymers enabled quantification of the glassy layer's thickness, which we relate to the strain softening (Payne effect), energy dissipation and the previously established nanostructure of the materials. We explored the thickness of the glassy layer from near the bulk glass transition temperature up to 363 K, in the presence or absence of nanoparticles and interfacially active polymers. Although the glassy layer becomes thinner with increasing temperature, it remains significant (> 3 nm) even when the sample is more than 180 K above the bulk glass transition temperature. This layer can account for the substantial levels of reinforcement, up to a factor of 20, and energy dissipation observed in silica filled rubbers beyond values expected from particle volume fraction arguments alone. Since the interfacially‐active polymers simultaneously inhibit nanoparticle aggregation and introduce polymer chain ends to the interparticle region, these experiments provide a direct test of whether energy loss in reinforced nanocomposites is attributable to “glassy bridges” between particles or chain ends. We show that while chain ends may be significant at low strain, below 1%, the percolation of the glassy layer of hindered polymer dynamics between silica particles dominates the Payne effect at high strain (~10% or more) and that this contribution can be dramatically reduced by sufficient steric stabilization to the nanoparticles.

Polymer CompositesVol. 47(1)
Science and Technology Facilities Council (GB), Durham University (GB), Institut Laue-Langevin (FR), University of Sheffield (GB)
Science and Technology Facilities Council
Openalex Percentile: Top 34%
Polymer Nanocomposites and Properties
0.61
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.