Effect of Silicon Carbide Additives on the Structure and Thermal Coefficient of Linear Expansion of a Composite Material Based on Al–Si Alloy

The results of dilatometric and structural studies of hypereutectic aluminum silicon alloys with a content of up to 30% silicon carbide in the test temperature range of 20–120°С are presented. The influence of modifying additives of silicon carbide on the nature of changes in the structure and temperature coefficient of linear expansion (TCLE) of the resulting composite is shown. The main technological conditions for obtaining the composite material of the Al–Si–SiC system are determined by sequential melting of aluminum at 660°С, followed by the addition of Al of 30% by weight SiC to the melt, by heating to 1250°С, and 10 min exposure and pouring the melt into the coquille, which allowed to obtain a composite material with TCLR 9.22 × 10–6 °С–1 in the specified temperature range.

Authors

Institutions

Publication Details

Journal
Surface Engineering and Applied Electrochemistry
Published
2025-05-01
DOI
https://doi.org/10.3103/s1068375525700292
Citations
1
Primary Topic
Aluminum Alloys Composites Properties
Type
article
Field-Weighted Citation Impact
0.71
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Effect of Silicon Carbide Additives on the Structure and Thermal Coefficient of Linear Expansion of a Composite Material Based on Al–Si Alloy

Л. В. Судник, В. И. Овчинников, K. F. Rudnitsky, V. N. Davydkin
1 citations
Surface Engineering and Applied Electrochemistry
Aluminum Alloys Composites Properties
0.71
article

Effect of Silicon Carbide Additives on the Structure and Thermal Coefficient of Linear Expansion of a Composite Material Based on Al–Si Alloy

Л. В. Судник, В. И. Овчинников, K. F. Rudnitsky, V. N. Davydkin
article en
1 citations

Abstract

The results of dilatometric and structural studies of hypereutectic aluminum silicon alloys with a content of up to 30% silicon carbide in the test temperature range of 20–120°С are presented. The influence of modifying additives of silicon carbide on the nature of changes in the structure and temperature coefficient of linear expansion (TCLE) of the resulting composite is shown. The main technological conditions for obtaining the composite material of the Al–Si–SiC system are determined by sequential melting of aluminum at 660°С, followed by the addition of Al of 30% by weight SiC to the melt, by heating to 1250°С, and 10 min exposure and pouring the melt into the coquille, which allowed to obtain a composite material with TCLR 9.22 × 10–6 °С–1 in the specified temperature range.

Surface Engineering and Applied ElectrochemistryVol. 61(3)
United Institute of Informatics Problems (BY)
Openalex Percentile: Top 30%
Aluminum Alloys Composites Properties
0.71
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.