Modulating Dynamic Deprotonation Evolution via Sacrificial Solvation Structure to Mitigate Zinc Electrochemical Corrosion and Cathodic Structure Deterioration for High‐Stable Zinc‐Vanadium Batteries

Compared to the free water molecules induced chemical corrosion, the electrochemical corrosion arising from the structured water elicits more pronounced zinc anode degradation, result in the limited cycle lifespan, especially at low current densities. However, the interfacial degradation mechanism remains inadequately resolved. Herein, for the inhibition of proton-induced side reactions, a lean-water polymer electrolyte is developed through the chelation of carboxymethyl chitosan (CCS) with Zn<sup>2+</sup> ions. In accordance with Fajans' rules, CCS with highly polar carboxylate and strong electron-withdrawing amino groups exhibits enhanced ionic polarizability, which forms distinctive solvation structures with reduced deprotonation energy. Such solvation structures demonstrate competitive advantages in interfacial deprotonation dynamics and minimize proton release to suppress electrochemical corrosion via sacrificial protection. Furthermore, the crosslinked framework induced by molecular crowding restricts free water mobility, thereby alleviating zinc chemical corrosion and cathodic structure deterioration. By employing advanced MRI technology, the movement trajectories of water molecules and the dynamic deprotonation evolution process are directly visualized. Therefore, the cyclically rested Zn symmetric cell impressively operates 4000 h at low current density of 0.1 mA cm<sup>-2</sup>. Additionally, the Zn||NH<sub>4</sub>VO full cell exhibits 81% capacity retention after cycling over 1000 cycles at 1 A g<sup>-1</sup>, while the aqueous electrolyte only maintains 31%.

Authors

Institutions

Publication Details

Journal
Advanced Materials
Published
2025-06-24
DOI
https://doi.org/10.1002/adma.202509622
Citations
13
Primary Topic
Advanced battery technologies research
Type
article
Field-Weighted Citation Impact
9.50

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Modulating Dynamic Deprotonation Evolution via Sacrificial Solvation Structure to Mitigate Zinc Electrochemical Corrosion and Cathodic Structure Deterioration for High‐Stable Zinc‐Vanadium Batteries

Kai Bai, Yongchao Tang, Zuyang Hu, Xiaolong Jiang et al.
13 citations
Advanced Materials
Advanced battery technologies research
9.50
article

Modulating Dynamic Deprotonation Evolution via Sacrificial Solvation Structure to Mitigate Zinc Electrochemical Corrosion and Cathodic Structure Deterioration for High‐Stable Zinc‐Vanadium Batteries

Kai Bai, Yongchao Tang, Zuyang Hu, Xiaolong Jiang, Wencheng Du, Chengchao Li, Minghui Ye, Zixin Han, Zhipeng Wen, Xiaoqing Liu, Yufei Zhang, Haoxin Liu, Junxi Chen
article en
13 citations

Abstract

Compared to the free water molecules induced chemical corrosion, the electrochemical corrosion arising from the structured water elicits more pronounced zinc anode degradation, result in the limited cycle lifespan, especially at low current densities. However, the interfacial degradation mechanism remains inadequately resolved. Herein, for the inhibition of proton-induced side reactions, a lean-water polymer electrolyte is developed through the chelation of carboxymethyl chitosan (CCS) with Zn<sup>2+</sup> ions. In accordance with Fajans' rules, CCS with highly polar carboxylate and strong electron-withdrawing amino groups exhibits enhanced ionic polarizability, which forms distinctive solvation structures with reduced deprotonation energy. Such solvation structures demonstrate competitive advantages in interfacial deprotonation dynamics and minimize proton release to suppress electrochemical corrosion via sacrificial protection. Furthermore, the crosslinked framework induced by molecular crowding restricts free water mobility, thereby alleviating zinc chemical corrosion and cathodic structure deterioration. By employing advanced MRI technology, the movement trajectories of water molecules and the dynamic deprotonation evolution process are directly visualized. Therefore, the cyclically rested Zn symmetric cell impressively operates 4000 h at low current density of 0.1 mA cm<sup>-2</sup>. Additionally, the Zn||NH<sub>4</sub>VO full cell exhibits 81% capacity retention after cycling over 1000 cycles at 1 A g<sup>-1</sup>, while the aqueous electrolyte only maintains 31%.

Advanced MaterialsVol. 37(40)
Guangdong University of Technology (CN), Ji Hua Laboratory (CN)
National Natural Science Foundation of China, Basic and Applied Basic Research Foundation of Guangdong Province
Openalex Percentile: Top 2%
Advanced battery technologies research
9.50
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.