Effect of Distribution of Substitution on Marine Biodegradability for Paramylon Acetate and Cellulose Acetate

Paramylon acetate and cellulose acetate with different degrees and distributions of substituents were synthesized by two different methods, de-esterification from triesters with NaOH treatment and direct esterification. Paramylon and cellulose acetate obtained by de-esterification exhibited a lower degree of substitution (DS) at C6 and a higher DS at C2 position. All of the acetate samples with different DSs were thermoformable, producing transparent films. However, melt-pressed films obtained through de-esterification exhibited greater flexibility than those prepared via direct esterification. Simultaneously, biochemical oxygen demand (BOD) tests demonstrated that paramylon and cellulose acetate obtained by de-esterification show higher biodegradability than esterification ones with the same DS. This increased biodegradability may be attributed to the lower DS of the acetyl group on C6 for paramylon and cellulose acetate obtained by de-esterification. De-esterification with NaOH treatment was validated as an effective approach for producing polysaccharide esters with excellent mechanical properties and biodegradability for both paramylon and cellulose.

Authors

Institutions

Publication Details

Journal
Biomacromolecules
Published
2025-06-13
DOI
https://doi.org/10.1021/acs.biomac.5c00252
Citations
3
Primary Topic
Microplastics and Plastic Pollution
Type
article
Field-Weighted Citation Impact
1.51

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Effect of Distribution of Substitution on Marine Biodegradability for Paramylon Acetate and Cellulose Acetate

Jin Ho Seok, Ruiqi Li, Tadahisa Iwata
3 citations
Biomacromolecules
Microplastics and Plastic Pollution
1.51
article

Effect of Distribution of Substitution on Marine Biodegradability for Paramylon Acetate and Cellulose Acetate

Jin Ho Seok, Ruiqi Li, Tadahisa Iwata
article en
3 citations

Abstract

Paramylon acetate and cellulose acetate with different degrees and distributions of substituents were synthesized by two different methods, de-esterification from triesters with NaOH treatment and direct esterification. Paramylon and cellulose acetate obtained by de-esterification exhibited a lower degree of substitution (DS) at C6 and a higher DS at C2 position. All of the acetate samples with different DSs were thermoformable, producing transparent films. However, melt-pressed films obtained through de-esterification exhibited greater flexibility than those prepared via direct esterification. Simultaneously, biochemical oxygen demand (BOD) tests demonstrated that paramylon and cellulose acetate obtained by de-esterification show higher biodegradability than esterification ones with the same DS. This increased biodegradability may be attributed to the lower DS of the acetyl group on C6 for paramylon and cellulose acetate obtained by de-esterification. De-esterification with NaOH treatment was validated as an effective approach for producing polysaccharide esters with excellent mechanical properties and biodegradability for both paramylon and cellulose.

BiomacromoleculesVol. 26(7)
The University of Tokyo (JP)
New Energy and Industrial Technology Development Organization
Openalex Percentile: Top 19%
Microplastics and Plastic Pollution
1.51
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Effect of Distribution of Substitution on Marine Biodegradability for Paramylon Acetate and Cellulose Acetate — Jin Ho Seok, Ruiqi Li, et al. · Biomacromolecules (2025) | TGRS Research Map | TGRS