NiMn2O4 Ceramic with Bi2O3 as Ablating Aid with Laser Melting Deposition

NiMn<sub>2</sub>O<sub>4</sub> thermosensitive ceramics using Bi<sub>2</sub>O<sub>3</sub> as a low-temperature ablating aid were prepared by laser melting deposition. Analyzing the structural, morphological, and electrical properties of the ceramics revealed important roles of Bi<sub>2</sub>O<sub>3</sub>. The room-temperature resistance decreased gradually with the increasing of the Bi<sub>2</sub>O<sub>3</sub> content, the thermal constant of the ceramics varied from 2870.1 to 3853.2 K, and the activation energy varied from 0.2473 to 0.3320 eV. Furthermore, the alleviation of the aging issue was attributed to the grain growth and the densification of the ceramics due to the addition of Bi<sub>2</sub>O<sub>3</sub> and the corresponding cationic redistribution. As a result, an optimized resistance drifting (∆R/R = 5.72%) of the ceramic was obtained with the addition of Bi<sub>2</sub>O<sub>3</sub>.

Authors

Institutions

Publication Details

Journal
Materials
Published
2025-05-30
DOI
https://doi.org/10.3390/ma18112571
Primary Topic
Electrical and Thermal Properties of Materials
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

NiMn2O4 Ceramic with Bi2O3 as Ablating Aid with Laser Melting Deposition

Shujian Ding, Weili Wang, Xiang Weng, Guang‐Hui Liu et al.
Materials
Electrical and Thermal Properties of Materials
article

NiMn2O4 Ceramic with Bi2O3 as Ablating Aid with Laser Melting Deposition

Shujian Ding, Weili Wang, Xiang Weng, Guang‐Hui Liu, Wei Ren, Yanhan Yang, Xian-Hai Liu
article en

Abstract

NiMn<sub>2</sub>O<sub>4</sub> thermosensitive ceramics using Bi<sub>2</sub>O<sub>3</sub> as a low-temperature ablating aid were prepared by laser melting deposition. Analyzing the structural, morphological, and electrical properties of the ceramics revealed important roles of Bi<sub>2</sub>O<sub>3</sub>. The room-temperature resistance decreased gradually with the increasing of the Bi<sub>2</sub>O<sub>3</sub> content, the thermal constant of the ceramics varied from 2870.1 to 3853.2 K, and the activation energy varied from 0.2473 to 0.3320 eV. Furthermore, the alleviation of the aging issue was attributed to the grain growth and the densification of the ceramics due to the addition of Bi<sub>2</sub>O<sub>3</sub> and the corresponding cationic redistribution. As a result, an optimized resistance drifting (∆R/R = 5.72%) of the ceramic was obtained with the addition of Bi<sub>2</sub>O<sub>3</sub>.

MaterialsVol. 18(11)
Northwestern Polytechnical University (CN), Xi’an University of Posts and Telecommunications (CN)
National Natural Science Foundation of China
Openalex Percentile: Top 90%
Electrical and Thermal Properties of Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.