Effect of glazing and hydrothermal aging on the fracture strength of metal-ceramic single restorations after additional firing: an in vitro study
Glazing does not significantly affect the fracture strength of a metal-ceramic crown undergoing additional firing; however, aging has a significant adverse effect on fracture strength. This negative effect is not significant until after 3 months.
Authors
- Mohammad Mahdi Parvizi (ORCID: https://orcid.org/0000-0003-1856-945X)
- Elham Ansarifard (ORCID: https://orcid.org/0000-0003-1532-8335)
- Masumeh Taghva (ORCID: https://orcid.org/0000-0001-6662-2257)
- Seyed Ali Mosaddad (ORCID: https://orcid.org/0000-0001-6963-8289)
Institutions
- Universidad Complutense de Madrid (ES)
- Shiraz University of Medical Sciences (IR)
- Shahid Sadoughi University of Medical Sciences and Health Services (IR)
- Saveetha University (IN)
Publication Details
- Journal
- BMC Oral Health
- Published
- 2025-05-28
- DOI
- https://doi.org/10.1186/s12903-025-05972-w
- Primary Topic
- Dental materials and restorations
- Type
- article
- Field-Weighted Citation Impact
- 0.00
Funders
- Shiraz University of Medical Sciences
- Shiraz University