Assessing shear bond strength of various surface treatments of titanium alloy with high translucency monolithic zirconia
The surface treatment of Ti6Al4V with either 50-µm alumina airborne-particle abrasion or 9.5% hydrofluoric acid improved the bond strength between Ti6Al4V and high translucent monolithic zirconia. Anodization did not improve the bond strength, regardless of the surface treatments.