Green Degumming of Hemp Fibers Using Ternary Deep Eutectic Solvents

As the demand for natural fibers grows to replace fossil-based alternatives, bast fibers including hemp, jute, and flax are considered the most viable complement to cotton; however, they require degumming, a process that removes gummy substances such as pectin, lignin, and hemicellulose to make them suitable for further use. Eco-friendly degumming is essential to minimize the use of harsh chemicals and water, reducing environmental impact while preserving the natural qualities of the fibers. This study explores the potential of two ternary deep eutectic solvents (DESs): choline chloride/lactic acid/glycerol and choline chloride/lactic acid/urea while comparing them against a binary DES (choline chloride/lactic acid) and traditional degumming, as a green alternative for degumming hemp fibers. Among the tested conditions, the choline chloride/lactic acid/glycerol (1:5:2) and choline chloride/lactic acid/urea (1:5:2) DES formulations, applied at 105 °C for 2 h with a 1:20 bath ratio, showed the most efficient degumming performance and preserved fiber quality. By optimizing treatment conditions, ternary DES systems demonstrated effective removal of noncellulosic components, leading to enhanced fiber separation, improved crystallinity, and superior tenacity compared to the traditional method within a quicker time. Structural and thermal analyses confirmed the preservation of cellulose integrity, while solvent recovery and reuse at least for 4 cycles further underscored the feasibility of this approach for scalable industrial applications. The calculation of cost for chemicals, energy, and water for 4 degumming cycles demonstrated that the DES process was more economical compared to traditional degumming. The findings highlight ternary DES as a promising solution for sustainable fiber processing, paving the way for future research on its application across diverse bast fibers and lignocellulosic resources.

Authors

Institutions

Publication Details

Journal
ACS Sustainable Chemistry & Engineering
Published
2025-05-19
DOI
https://doi.org/10.1021/acssuschemeng.5c02405
Citations
6
Primary Topic
Advanced Cellulose Research Studies
Type
article
Field-Weighted Citation Impact
3.58

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Green Degumming of Hemp Fibers Using Ternary Deep Eutectic Solvents

Mina Bayattork, Abu Naser Md Ahsanul Haque, Maryam Naebe, Yi Zhang
6 citations
ACS Sustainable Chemistry & Engineering
Advanced Cellulose Research Studies
3.58
article

Green Degumming of Hemp Fibers Using Ternary Deep Eutectic Solvents

Mina Bayattork, Abu Naser Md Ahsanul Haque, Maryam Naebe, Yi Zhang
article en
6 citations

Abstract

As the demand for natural fibers grows to replace fossil-based alternatives, bast fibers including hemp, jute, and flax are considered the most viable complement to cotton; however, they require degumming, a process that removes gummy substances such as pectin, lignin, and hemicellulose to make them suitable for further use. Eco-friendly degumming is essential to minimize the use of harsh chemicals and water, reducing environmental impact while preserving the natural qualities of the fibers. This study explores the potential of two ternary deep eutectic solvents (DESs): choline chloride/lactic acid/glycerol and choline chloride/lactic acid/urea while comparing them against a binary DES (choline chloride/lactic acid) and traditional degumming, as a green alternative for degumming hemp fibers. Among the tested conditions, the choline chloride/lactic acid/glycerol (1:5:2) and choline chloride/lactic acid/urea (1:5:2) DES formulations, applied at 105 °C for 2 h with a 1:20 bath ratio, showed the most efficient degumming performance and preserved fiber quality. By optimizing treatment conditions, ternary DES systems demonstrated effective removal of noncellulosic components, leading to enhanced fiber separation, improved crystallinity, and superior tenacity compared to the traditional method within a quicker time. Structural and thermal analyses confirmed the preservation of cellulose integrity, while solvent recovery and reuse at least for 4 cycles further underscored the feasibility of this approach for scalable industrial applications. The calculation of cost for chemicals, energy, and water for 4 degumming cycles demonstrated that the DES process was more economical compared to traditional degumming. The findings highlight ternary DES as a promising solution for sustainable fiber processing, paving the way for future research on its application across diverse bast fibers and lignocellulosic resources.

ACS Sustainable Chemistry & EngineeringVol. 13(21)
Deakin University (AU)
Australian Research Council
Openalex Percentile: Top 7%
Advanced Cellulose Research Studies
3.58
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.